Enamel loss following ceramic bracket debonding: A quantitative analysis in vitro
- 1 July 2015
- journal article
- research article
- Published by The Angle Orthodontist (EH Angle Education & Research Foundation) in The Angle Orthodontist
- Vol. 85 (4) , 651-656
Abstract
Objective: : To measure enamel surface changes after ceramic bracket debonding and after cleanup. Materials and Methods: : Forty extracted teeth were scanned in three dimensions using an optical scanner (baseline). Two ceramic bracket systems were placed (19 metal-reinforced polycrystalline ceramic brackets; 21 monocrystalline ceramic brackets). Seven days later, brackets were debonded and teeth scanned (post-debond). Adhesive remnants and bracket fragments were recorded. Tooth surfaces were cleaned using a finishing carbide bur and scanned again (post-cleanup). Post-debond and post-cleanup scans were aligned with the baseline, and surface changes were quantified. Results were statistically compared using t -tests and Mann-Whitney tests (α = .05). Results: : The depth of enamel loss (mean ± standard deviation) post-debond was 21 ± 8 µm and 33 µm and post-cleanup was 28 ± 14 µm and 18 ± 8 µm ( P = .0191); the post-debond remnant thickness was 188 ± 113 µm and 120 ± 37 µm ( P = .2381) and post-cleanup was 16 ± 5 µm and 15 µm for polycrystalline and monocrystalline ceramic brackets, respectively. The monocrystalline ceramic brackets predominantly left all adhesive on the tooth; the polycrystalline ceramic brackets were more likely to leave bracket fragments attached. Conclusion: : Both systems allowed successful removal of the brackets with minimal enamel loss. However, the polycrystalline ceramic brackets left more fragments on the tooth, which complicated cleanup efforts.Keywords
This publication has 19 references indexed in Scilit:
- Enamel loss and adhesive remnants following bracket removal and various clean-up procedures in vitroEuropean Journal of Orthodontics, 2011
- Three-dimensional quantification of adhesive remnants on teeth after debondingAmerican Journal of Orthodontics and Dentofacial Orthopedics, 2008
- Three-dimensional measurement of residual adhesive and enamel loss on teeth after debonding of orthodontic brackets: An in-vitro studyAmerican Journal of Orthodontics and Dentofacial Orthopedics, 2007
- Ceramic brackets: Something old, something new, a reviewSeminars in Orthodontics, 1997
- A post-treatment evaluation of multibonded ceramic brackets in orthodonticsEuropean Journal of Orthodontics, 1997
- Enamel fracture caused by ceramic bracketsAmerican Journal of Orthodontics and Dentofacial Orthopedics, 1991
- Measurement of change in surface contour by computer graphicsDental Materials, 1985
- Clinical trials with crystal growth conditioning as an alternative to acid-etch enamel pretreatmentAmerican Journal of Orthodontics, 1984
- Use of Epoxy Resins in Restorative MaterialsJournal of Dental Research, 1956
- A Simple Method of Increasing the Adhesion of Acrylic Filling Materials to Enamel SurfacesJournal of Dental Research, 1955