Abstract
Low-rank ultrafine flotation clean coal typically yields filter cake moisture above 20% due to abundant oxygen-containing functional groups and strong surface hydrophilicity. Conventional polyacrylamide (PAM) flocculants are hydrophilic and improve dewatering only by altering cake porosity, not by reducing particle surface hydrophilicity, so they remove little adsorbed water. In this study, hydrophobically modified anionic polyacrylamides (HMAPAM) were synthesized by grafting lauryl acrylate onto APAM. FTIR, 1H NMR, XPS, and SEM confirmed the grafting and progressive enrichment of hydrophobic alkyl chains on the surface. Moderate hydrophobic modification markedly improved solid–liquid separation. HMAPAM-D (APAM/LA = 4.5:0.5) achieved a settling velocity of 0.817 cm/s at 9 mg/L, 50.2% higher than APAM, and reduced filter cake moisture to 16.64% at 1 mg/L under 0.6 MPa versus 19.39% for unmodified APAM. Excessive modification (HMAPAM-E, 4:1) promoted intramolecular self-association, producing heterogeneous flocs and higher filtration resistance that degraded dewatering efficiency. The performance gain stems from hydrophobic association combined with adsorption bridging. These results clarify how hydrophobic group content controls flocculation and dewatering, informing the design of better flocculants for this type of coal slurry.
Funding Information
  • National Key Research and Development Program of China (2024YFC2909800)
  • Fundamental Research Funds for the Central Universities (2025ZKPYHH03)

This publication has 34 references indexed in Scilit: