Abstract
Defects induced by B+ implantation (35 keV) at liquid‐nitrogen (LN) temperature and −60 °C are examined using transmission electron microscopy (TEM), secondary‐ion‐mass spectroscopy, and electrical characterization of p+n diodes. B+ implantation at LN temperature produces a 120‐nm‐thick amorphous layer with a residual surface crystalline region. B+ implantation at −60 °C does not produce an amorphous layer, but damage can be observed as a dark band at the depth of B+ projected range Rp. For RT implantation, cross‐sectional transmission electron microscopy reveals no visible damage in contrast to implantation at −60 °C. Frenkel‐pair diffusion and annihilation is suppressed during implantation at the low temperature. The damage accumulates to form an amorphous layer for LN temperature. At −60 °C, the defects are confined near Rp. After annealing at 1000 °C for 10 min, near‐surface and depth‐encountering solid‐phase‐epitaxy dislocation‐loop defects are observed in the sample implanted at LN temperature. The density of these is about several 108 cm−2, which is 10 or 100 times smaller than samples implanted at higher temperature. The annealed samples implanted at −60 °C and RT are mainly 〈111〉‐plane directed defects and dislocation loops, respectively. Corresponding to the degree of as‐implanted damage, the defects distribute at a shallower depth in the sample implanted at −60 °C than at RT, and have about 10 times higher density. The leakage current characteristics of p+n diodes indicate that the LN temperature and −60 °C implanted samples have lower leakage than RT samples at all annealing conditions. Notably, at 1000 °C for 10 min the leakage current is reduced to 56%. This is consistent with the result of TEM analysis; thus, the defect confinement to shallow layer by cooling contributes to lower the leakage current. Implantation at −60 °C is suitable for modern high‐current implanters, due to practical coolant and less mechanical stress by thermoplasticity.Keywords
This publication has 28 references indexed in Scilit:
- Defects production and annealing in self-implanted SiJournal of Applied Physics, 1991
- Structural characterization of damage in Si(100) produced by MeV Si+ion implantation and annealingJournal of Materials Research, 1990
- New method of solid state wafer cooling in the Extrion 1000 high current ion implantation systemNuclear Instruments and Methods in Physics Research Section B: Beam Interactions with Materials and Atoms, 1989
- Temperature Dependence of Damage in Boron-Implanted SiliconMRS Proceedings, 1989
- Damage Growth in Si During Self-Ion Irradiation: a Study of Ion Effects Over an Extended Energy RangeMRS Proceedings, 1989
- Elimination of end-of-range and mask edge lateral damage in Ge+ preamorphized, B+ implanted SiApplied Physics Letters, 1986
- Kinetics of damage production in silicon during self-implantationJournal of Applied Physics, 1986
- Characteristics of Ion‐Implantation Damage and Annealing Phenomena in SemiconductorsJournal of the Electrochemical Society, 1984
- Substrate-orientation dependence of the epitaxial regrowth rate from Si-implanted amorphous SiJournal of Applied Physics, 1978
- Crystalline to amorphous transformation in ion-implanted silicon: a composite modelJournal of Applied Physics, 1978