Results of pulsed field antiferromagnetic resonance (AFMR) experiments are briefly summarized for the mixed crystal system (Cr2O3)1−x·(Al2O3)x as a function of temperature, and X , where X = 0.003 , 0.006, 0.008, 0.06, 0.1, 0.2, and 0.9. The temperature dependence of the critical field, (2λK)12 , for pure Cr2O3 and X = 0.1 are compared in detail. The increase of (2λK)12 at 4.2°K from about 59 kilogauss for Cr2O3 to 79 kilogauss for X = 0.1 is attributed to a reversal in sign and rapid increase in magnitude of the effective crystalline field contribution to the anisotropy energy as X is increased. AFMR linewidths from 800 to 2000 gauss were observed, but for X≤0.2 the linewidth was almost independent of temperature for each composition. The decrease of Néel temperature with increase of X is also summarized.