First result of boronization assisted by the ICWC on EAST with full metal wall
Authors:
- Y.H. GuanYGY.H. Guan
- G Z ZuoGZG Z Zuo
- W XuWXW Xu
- Yaowei YuYYYaowei Yu
- Zhen SunZSZhen Sun
- Zhe WangZWZhe Wang
- Rui DingRDRui Ding
- Ling ZhangLZLing Zhang
- Zhenwei WuZWZhenwei Wu
- Songtao MaoSMSongtao Mao
- Hailin ZhaoHZHailin Zhao
Open Access
- 4 August 2025
- journal article
- Published by IOP Publishing in Nuclear Fusion
- Vol. 65 (9)
Abstract
Boron (B), a low-Z (atomic number) material, has been widely utilized in wall conditioning to improve plasma performance in fusion devices [1]. In 2023, boronization was successfully conducted on EAST featuring an ITER-like tungsten divertor and fully metallic first wall. The process employed predischarge coating with carborane (C2B10H12) as the working material, assisted by ion cyclotron wall conditioning (ICWC). After one time 12 g boronization, it was found the thickness of B film was approximately 120 nm. Post-boronization observations indicated that substantial hydrogen (H) release during initial plasma discharges compared with the consumed W/B wall, attributed to H co-deposition during the ICWC-boronization processing, which led to uncontrollable divertor neutral pressure and plasma density. The H/(H+D) ratio demonstrated a gradual reduction from ~85% to 30% over more than 1850 s of deuterium plasma, with a cumulative injected energy of 2325 MJ. The B coating significantly enhanced the stored energy in plasma and improved confinement performance. The stored energy in plasma showed an increase of about 20%, primarily due to a reduction in impurity radiation, including oxygen (O) and heavy impurities such as tungsten (W), iron (Fe), and copper (Cu). The effective ion charge (Zeff) decreased from 2.3 to 2.0. Following ICWC-boronization, the line-integrated radiation profile decreased by nearly 35% in the plasma core, plasma density and electron temperature exhibited an increase of ~7% and 12% due to enhanced wall fueling and reduced impurity radiation. The lifetime of boronization, as evaluated by the line emissions from boron and other impurity radiation, was about 1700 seconds of deuterium plasma, with a cumulative injected energy of 2125 MJ on EAST. These findings provide significant insights for evaluating ICWC-boronization applicability in ITER with full W wall structure.Keywords
Funding Information
- National Natural Science Foundation of China (12475208)
- National Key Research and Development Program of China (2022YFE03130000)
- National Key Research and Development Program of China (2024YFE03000200)
This publication has 63 references indexed in Scilit:
- An overview of lithium experiments on HT-7 and EAST during 2012Fusion Engineering and Design, 2014
- The WEST project: Testing ITER divertor high heat flux component technology in a steady state tokamak environmentFusion Engineering and Design, 2014
- Recent progress of NSTX lithium program and opportunities for magnetic fusion researchFusion Engineering and Design, 2011
- First boronization in KSTARFusion Engineering and Design, 2010
- Wall conditioning in ASDEX UpgradeJournal of Nuclear Materials, 2007
- An ITER-like wall for JETJournal of Nuclear Materials, 2007
- Impurity and particle recycling reduction by boronization in JT-60UJournal of Nuclear Materials, 1995
- Boronization of ASDEXJournal of Nuclear Materials, 1990
- Effects of light-ion irradiation on mechanical properties of metals and alloysJournal of Nuclear Materials, 1990
- Boronization in textorJournal of Nuclear Materials, 1989