Micro-Incremental Forming of Ti and Au Foils by Indentation Method
Authors:
- 15 August 2007
- journal article
- Published by Trans Tech Publications, Ltd. in Key Engineering Materials
- Vol. 345-346, 1101-1104
Abstract
Ti and Au foils with a thickness of 10μm were formed by indenting at a place neighboring another indented place sequentially by means of a hemispherical diamond tool with a radius of 5μm. In this forming method, forming dies are not necessary and commercial equipments for nanoindentation can be used. Forming load and pitch were changed in single line forming and forming direction, line pitch and line number were changed in plural line forming, and bending angle was investigated. From the experimental results, bending angle of Ti foil was greater than that of Au one when same working conditions were employed. As the forming pitch increased, bending angle decreased. When the forming line pitch was changed, bending angle had the maximum peak at a pitch of 30μm by one-way forming path and 25μm by two-way forming path. Bending angle by one-way forming path was larger than that by two-way forming path. As forming line number increased, although bending angle increased, increment of them became smaller.Keywords
This publication has 3 references indexed in Scilit:
- Flexible Sheet Forming Technology by Double-sided Simultaneous Shot Peen FormingCIRP Annals, 2002
- An in-situ incremental microforming system for three-dimensional shell structures of foil materialsJournal of Materials Processing Technology, 2001
- Microdeep drawability of very thin sheet steelsJournal of Materials Processing Technology, 2001