Abstract
La0.6Sr0.4Co0.2Fe0.8O3-Ce0.9Gd0.1O1.95 (LSCF-GDC) nanocomposite cathode material has been synthesized using a simple combustion process for intermediate and low temperature solid oxide fuel cells (SOFCs). The combusted cathode material was calcined at temperatures 600, 700 and 800 C/2 h. The powder properties such as evolution of crystalline phases, thermal decomposition, BET surface area, particle size and morphology are analyzed and reported. The TEM images confirmed that the cathode material has uniform eqiaxial shape and nanometric crystallite size of range from 15 to 45 nm. The electrical conductivity of the sintered LSCF-GDC cathode was examined. Subsequently, the cathode material was applied on GDC electrolyte to obtain a half-cell (electrode/electrolyte structure) configuration. The electrical properties of the half-cell at different temperatures were studied and discussed.