Sintering Behavior, Microstructure, and Phase Composition of Sr(Fe,Co)O 3−δ Ceramics
Authors:
- 20 December 2000
- journal article
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 83 (12) , 3158-3164
Abstract
SrFe 1− x Co x O 3−δ ( x = 0, 0.33) ceramics have been prepared in the temperature interval 900–1350°C in air, nitrogen, and oxygen atmosphere. The effect of cation nonstoichiometry on densification behavior, microstructure, and phase composition has been investigated. Densification of Sr‐deficient SrFeO 3−δ initiates at a lower temperature than near stoichiometric SrFeO 3−δ probably due to enhanced diffusion of Sr. However, for Sr‐deficient samples Sr 4 Fe 6 O 13 is formed above ∼775°C, causing a significant decrease in the sintering rate. It is therefore necessary to avoid Sr deficiency to obtain dense SrFeO 3−δ ceramics. The densification rate was significantly increased by Co substitution. Dense ceramics (>95% of theoretical density) of Sr‐excess and Co‐substituted SrFeO 3−δ were obtained by sintering in the temperature region 1000–1200°C. The grain size increases by increasing temperature, decreasing partial pressure of oxygen and Co substitution. Exaggerated grain growth in the Co‐substituted material occurred at high temperatures. Sintering above 1200°C caused all materials, apart from Co‐substituted SrFeO 3−δ in oxygen, to swell and develop a porous microstructure. The swelling mechanism was related to heterogeneous phase equilibria, which is reductive in nature and leads to evolution of oxygen gas. The phase equilibria are governed by the cation nonstoichiometry of the materials. The present findings demonstrate the importance of controlling the cation stoichiometry of ternary transition‐metal oxides to achieve ceramics with the desired homogeneous microstructure. The mixed valence state of the transition metal may lead to both swelling during sintering and cracking during cooling due to reduction/oxidation during heating/cooling.Keywords
This publication has 16 references indexed in Scilit:
- Ceramic Microstructure and Oxygen Permeability of SrCo ( Fe , M ) O 3 − δ ( M = Cu or Cr ) Perovskite MembranesJournal of the Electrochemical Society, 1998
- Materials of high-temperature electrochemical oxygen membranesJournal of Membrane Science, 1996
- Nonstoichiometry and phase relationship of the SrFeO2.5SrFeO3 system at high temperatureJournal of Solid State Chemistry, 1992
- Dependence of the structure and electronic state of SrFeOx (2.5 ≤ x ≤ 3) on composition and temperatureJournal of Solid State Chemistry, 1988
- Phase relation in the oxygen nonstoichiometric system, SrFeOx (2.5 ≤ x ≤ 3.0)Journal of Solid State Chemistry, 1986
- Structural transitions at high temperature in Sr2Fe2O5Journal of Solid State Chemistry, 1985
- Sintering Atmosphere Effects on the Ductility of W- Ni- Fe Heavy MetalsMetallurgical Transactions A, 1984
- The SrFeO2.5 | SrFeO3.0 system. Evidence of a new phase Sr4Fe4O11 (SrFeO2.75)Materials Research Bulletin, 1975
- A powder neutron diffraction investigation of the nuclear and magnetic structure of Sr2Fe2O5Acta Crystallographica Section B: Structural Science, Crystal Engineering and Materials, 1975
- Effective ionic radii in oxides and fluoridesActa Crystallographica Section B: Structural Science, Crystal Engineering and Materials, 1969