The influence of Ni on the composition, structure and properties of Ti-Cr-N coatings
Open Access
- 15 March 2023
- journal article
- research article
- Published by National University of Science and Technology MISiS in Powder Metallurgy аnd Functional Coatings
- No. 1,p. 63-74
Abstract
The influence of nickel on the structure and properties of Ti-Cr-N ion-plasma coatings obtained by arc-PVD method has been studied. With a nickel content of up to 11.9 at. %, the coating consists of Cr2N, Ti1 – xCrxN, and metallic Ni. Upon further increase in Ni concentration in the coating, intermetallic compound Ni3Ti is formed. The structure of the coatings was studied using the transmission electron microscopy. The coatings of Ti-Cr-N system are characterized by a columnar structure, in the columns of which Ti1 - xCrxN and Ti1 - yCryN (x > y) sublayers, being several nanometers thick and containing variable concentration of titanium and chromium, as well as Cr2N sublayers of about 25 nm are formed due to the complete solubility of TiN and Cr2N and the planetary rotation of the substrates, resulting in layer-by-layer stacking of the components of the evaporated cathodes. This structure remains intact in coatings of Ti-Cr-N-Ni system with a low nickel concentration (on the order of tenths of at. %). However, upon that, the column size refinement and an increase in biaxial compressive stresses from 6.7 to 9.7 GPa are observed, which results in an increase in hardness from 30 to 42 GPa. The coatings with a high nickel content are characterized by a multilayer architecture with an equiaxed polycrystalline structure of nanograins in layers. As Ni concentration increases, the hardness of the coating decreases to 16.7 GPa, which is associated with an increase in the fraction of relatively soft nickel in the coating and a decrease in macrostresses to -0.6 GPa. Upon that, the wear intensity increases from 3·10-15 to 5·10-15 m3/(N·m). The studied coatings of Ti–Cr–N and Ti–Cr–N–Ni systems are resistant to adhesive and cohesive destruction. With an increase in the nickel content upon measuring scratching, the destruction of the coatings occurs exclusively due to the plastic deformation.Keywords
This publication has 24 references indexed in Scilit:
- Structure and mechanical stability of molybdenum nitrides: A first-principles studyPhysical Review B, 2007
- XPS investigations of chromium nitride thin filmsSurface and Coatings Technology, 2005
- Different approaches to superhard coatings and nanocompositesThin Solid Films, 2005
- Preparation and Characterization of CrN/CN and Nano‐TiN/CN CompositesJournal of the American Ceramic Society, 2005
- Influence of nitrogen content on the structural, mechanical and electrical properties of TiN thin filmsSurface and Coatings Technology, 2005
- Effect of nitrogen pressure, bias voltage and substrate temperature on the phase structure of Mo–N coatings produced by cathodic arc PVDSurface and Coatings Technology, 2003
- Oxidation kinetics of sputtered Cr–N hard coatingsSurface and Coatings Technology, 2001
- Thermodynamic properties of ni nitrides and phase stability in the Ni-N systemInternational Journal of Thermophysics, 1991
- A thermodynamic evaluation of the Cr-N, Fe-N, Mo-N and Cr-Mo-N systemsCalphad, 1991
- The Mo-N (Molybdenum-Nitrogen) systemBulletin of Alloy Phase Diagrams, 1980