Abstract
In this work, we present experimental results examining the energy distribution of the relatively high (1×1011cm−2)(1×1011cm−2) electrically active interface defects which are commonly observed in high-dielectric-constant (high- kk ) metal–insulator–silicon systems during high- kk process development. This paper extends previous studies on the Si(100)∕SiOx∕HfO2Si(100)∕SiOx∕HfO2 system to include a comparative analysis of the density and energy distribution of interface defects for HfO2HfO2 , lanthanum silicate (LaSiOx)(LaSiOx) , and Gd2O3Gd2O3 thin films on (100) orientation silicon formed by a range of deposition techniques. The analysis of the interface defect density across the energy gap, for samples which experience no H2∕N2H2∕N2 annealing following the gate stack formation, reveals a peak density ( ∼2×1012cm−2eV−1∼2×1012cm−2eV−1 to ∼1×1013cm−2eV−1∼1×1013cm−2eV−1 ) at 0.83–0.92eV0.83–0.92eV above the silicon valence bandedge for the HfO2HfO2 , LaSiOxLaSiOx , and Gd2O3Gd2O3 thin films on Si(100)Si(100) . The characteristic peak in the interface state density (0.83–0.92eV)(0.83–0.92eV) is obtained for samples where no interface silicon oxide layer is observed from transmission electron microscopy. Analysis suggests silicon dangling bond (Pbo)(Pbo) centers as the common origin for the dominant interface defects for the various Si(100)∕SiOxSi(100)∕SiOx /high- kk /metal gate systems. The results of forming gas (H2∕N2)(H2∕N2) annealing over the temperature range 350–555°C350–555°C are presented and indicate interface state density reduction, as expected for silicon dangling bond centers. The technological relevance of the results is discussed.Keywords
This publication has 50 references indexed in Scilit:
- On the scaling issues and high-κ replacement of ultrathin gate dielectrics for nanoscale MOS transistorsMicroelectronic Engineering, 2006
- Impact of H2/N2 annealing on interface defect densities in Si(100)/SiO2/HfO2/TiN gate stacksMicroelectronic Engineering, 2005
- Carrier mobility in advanced CMOS devices with metal gate and HfO2 gate dielectricSolid-State Electronics, 2003
- Passivation and interface state density of SiO2/HfO2-based/polycrystalline-Si gate stacksApplied Physics Letters, 2003
- Origin of the threshold voltage instability in SiO2/HfO2 dual layer gate dielectricsIEEE Electron Device Letters, 2003
- Analysis of Pb centers at the Si(111)/SiO2 interface following rapid thermal annealingJournal of Applied Physics, 2003
- Characterization of La[sub 2]O[sub 3] and Yb[sub 2]O[sub 3] Thin Films for High-k Gate Insulator ApplicationJournal of the Electrochemical Society, 2003
- Defects at the interface of ultra-thin VUV-grown oxide on Si studied by electron spin resonanceApplied Surface Science, 2000
- Interface traps and P b centers in oxidized (100) silicon wafersApplied Physics Letters, 1986
- Strain broadening of the dangling-bond resonance at the (111)Si-interfacePhysical Review B, 1986