Degradation by acetic acid for crystalline Si photovoltaic modules
Authors:
- 12 March 2015
- journal article
- Published by IOP Publishing in Japanese Journal of Applied Physics
- Vol. 54 (4S) , 04DR04
Abstract
The degradation of crystalline Si photovoltaic modules during damp-heat test was studied using some test modules with and without polymer film insertion by observing electrical and electroluminescence properties and by chemical analyses. Acetic acid generated by the hydrolysis decomposition of ethylene vinyl acetate used as an encapsulant is the main origin of degradation. The change in electroluminescence images is explained on the basis of the corrosion of electrodes by acetic acid. On the other hand, little change was observed at the pn junction even after damp-heat test for a long time. Therefore, carrier generation occurs even after degradation; however, such generated carriers cannot be collected owing to corrosion of electrodes. The guiding principle that module structure and module materials without saving acetic acid into the modules was obtained.Keywords
This publication has 34 references indexed in Scilit:
- Systematic investigation of cracks in encapsulated solar cells after mechanical loadingSolar Energy Materials and Solar Cells, 2013
- On the mechanism of potential‐induced degradation in crystalline silicon solar cellsPhysica Status Solidi (RRL) – Rapid Research Letters, 2012
- Micro Structural Root Cause Analysis of Potential Induced Degradation in c-Si Solar CellsEnergy Procedia, 2012
- Durability of Pb‐free solder between copper interconnect and silicon in photovoltaic cellsProgress in Photovoltaics: Research and Applications, 2010
- History of accelerated and qualification testing of terrestrial photovoltaic modules: A literature reviewProgress in Photovoltaics: Research and Applications, 2008
- Acetic acid production and glass transition concerns with ethylene-vinyl acetate used in photovoltaic devicesSolar Energy Materials and Solar Cells, 2007
- Modeling of rates of moisture ingress into photovoltaic modulesSolar Energy Materials and Solar Cells, 2006
- Moisture sensor at glass/polymer interface for monitoring of photovoltaic module encapsulantsSensors and Actuators A: Physical, 2006
- The performance of crystalline silicon photovoltaic solar modules after 22 years of continuous outdoor exposureProgress in Photovoltaics: Research and Applications, 2005
- Thermal degradation of ethylene‐vinyl acetate copolymerJournal of Polymer Science Part C: Polymer Letters, 1973