Microhardness and Chemical Composition of Glass Ionomer and Glass Hybrid Cements Modified with Experimental Bioactive Glasses
Open Access
- 15 June 2026
- journal article
- Published by University of Zagreb School of Dental Medicine in Acta Stomatologica Croatica
- Vol. 60 (2) , 158-172
Abstract
The purpose of this in vitro study was to evaluate the effect of bioactive glasses containing a small proportion of fluoride and zinc in lower (BAG1) and higher ratios (BAG2) on the Vickers microhardness (VHN), surface morphology and chemical composition of high-viscosity glass ionomer cement and glass hybrid cement. Fuji IX (Fuji) and Equia Forte HT (Equia) were modified with 5 wt% BAG1 and BAG2. Six groups were prepared and stored in distilled water: Fuji, Fuji+ BAG1, Fuji+BAG2, Equia, Equia+ BAG1, and Equia+BAG2. BAG1 and BAG2 were characterized using FTIR. VHN was measured after 24 hours and 7 days. Representative samples from all groups were stored in phosphate buffered solution and analyzed using SEM-EDS. Data were analyzed using ANOVA and paired t-tests (α = 0.05). Fuji and Fuji+BAG1 showed the highest VHN at both time points, whereas BAG2 significantly reduced microhardness compared to original materials Fuji and Equia (p<0.05). All groups exhibited increased VHN over 7 days (p<0.05). FTIR confirmed the amorphous silicate and fluoride content. SEM-EDS confirmed the absence of crystalline precipitates on the material's surface when stored in phosphate containing solution. BAG1 preserved or slightly enhanced microhardness, while BAG2 significantly reduced it. There were no crystalline precipitates on original or on materials modified with 5 wt% bioactive glass. Optimizing BAG composition is essential to balance mechanical stability and bioactivity of glass ionomers.Keywords
This publication has 41 references indexed in Scilit:
- Evaluation of surface roughness and hardness of different glass ionomer cementsEuropean Journal of Dentistry, 2012
- Influence of strontium for calcium substitution in bioactive glasses on degradation, ion release and apatite formationJournal of The Royal Society Interface, 2011
- Glass ionomer cements and their role in the restoration of non-carious cervical lesionsJournal of Applied Oral Science, 2009
- Compressive strength and surface characterization of glass ionomer cements modified by particles of bioactive glassDental Materials, 2005
- Two‐body and three‐body wear of glass ionomer cementsInternational Journal of Paediatric Dentistry, 2003
- Effects of added bioactive glass on the setting and mechanical properties of resin-modified glass ionomer cementBiomaterials, 2003
- Short-term fluoride and cations release from polyacid-modified composites in a distilled water, and an acidic lactate bufferBiomaterials, 2003
- The Mechanism for Erosion of Glass-ionomer Cements in Organic-Acid Buffer SolutionsJournal of Dental Research, 1990
- Acid Reactivity of Carbonated Apatites with Strontium and Fluoride SubstitutionsJournal of Dental Research, 1983
- The clinical development of the glass‐ionomer cements. I. Formulations and properties*Australian Dental Journal, 1977