Identification and Formation Mechanism of a Deformation Process Determining Microstructure of Type IV Creep Damage of the Advanced High Cr Containing Ferritic Heat Resistant Steel
Authors:
Open Access
- 1 January 2006
- journal article
- Published by Iron and Steel Institute of Japan in Tetsu-to-Hagane
- Vol. 92 (10) , 609-617
Abstract
The microstructure of a Type IV damage, a ductile and early creep failure at outer edge of Heat Affected Zone of weld, was precisely researched. The rupture life of a simulated fine grain area of HAZ was the shortest compared with those of the other microstructures, coarse grain HAZ and dual phase HAZ, according to the temperature acceleration creep test at 700°C. The tensile strength at room temperature was the lowest at around Ac1 transformation point, determined by rapid heating diratometry. Therefore, the Type IV damage did not coincident the conventional HAZ softening phenomenon often observed in low carbon steels. Dislocation substructure of the fine grain zone is composed of the globular sub-grain microstructure and the coarsened carbide through the Transmission Electron Microscope observation of thin foils. They were possibly explained to be formed through the thermal cycle of HAZ and Post Weld Heat Treatment as follows: a base metal with lath martensite microstructure is warmed above Ac3 point once, and immediately cooled and transformed. Such "weak" lath martensite structure, apparent ambiguous lath martensite, was easily recovered to the globular sub-grain microstructure. Based on the hypothesis above mentioned, globular sub-grain microstructure at fine grain HAZ possibly resulted in the decrease of the creep life.Keywords
This publication has 8 references indexed in Scilit:
- Effect of Heat Treatment on Creep Properties and Microstructures of HAZ for 9%Cr Ferritic SteelJournal of the Society of Materials Science, Japan, 2003
- Creep Damage Development of a 1.25Cr-0.5Mo Steel Weldment Exposed to Long Term ServiceTetsu-to-Hagane, 2002
- Microstructures and Creep Strength of Welded Joints for W Strengthened High Cr Ferritic SteelJournal of the Society of Materials Science, Japan, 2001
- Bound volumes available to subscribersGastrointestinal Endoscopy, 2000
- Type IV Cracking and Life Evaluation of Weldments on 2.25Cr-1Mo Steel under Creep-Fatigue Loading ConditionJournal of the Society of Materials Science, Japan, 1999
- Residual Creep Life Assessment by Change of Martensitic Lath Structure in Modified 9Cr-1Mo SteelsTetsu-to-Hagane, 1998
- Current practice in China1994
- The behaviour of ferritic weldments in thick section pipe at elevated temperatureInternational Journal of Pressure Vessels and Piping, 1985