Abstract
Electrons trapped in the HfSiON gate dielectrics of n -channel metal-oxide-semiconductor field-effect transistors induced by positive bias temperature stress start to decay when the stress is interrupted or an opposite (recovery) voltage is applied. The decay begins with a quick detrapping within tens of nanoseconds followed by a slow detrapping. The quick detrapping depends on the recovery voltage and the trapping history, whereas the slow detrapping obeys approximately a logarithmic dependence on time with an almost identical slope before saturation. The observed detrapping behavior can be explained by a spatial and/or energetic distribution of trapped electrons in the HfSiON film. The device degradation under various dynamic stresses is found to be almost independent of frequency ranging from 0.001to1MHz , while it is slightly enhanced at 10MHz , probably due to insufficient recovery at the recovering half cycle.