Abstract
Effect of CaO and SiO 2 additions on the grain growth and magnetic and electrical properties of a Ni–Zn ferrite was studied. The common oxides ( x = 0.4CaO + 0.8SiO 2 ) were added in different moles ( x = 0, 0.02, 0.06, 0.012, 0.24 and 0.48) to Fe 2 O 3 , Zn, and NiO. The mixed powders were mechanically alloyed for 12 h using a high energy ball mill before heating at 1200 °C for 240 min. The products were characterized by x-ray diffraction (XRD), field emission scanning electron microscopy, energy-dispersive x-ray spectroscopy, vibrating sample magnetometer and static hysteresisgraph, and later by an impedance analyzer with a frequency range from 1 MHz to 1.8 GHz. The XRD results indicate a formation of single phase spinel structure in all the samples. The average grain size was affected by the additive contents so that their sizes grew, up to x = 0.06, and after that their sizes reduced from 0.631 to 0.371 μ at x = 0.48. The experimental density of the samples displayed an upward trend for x < 0.06, increasing from 5.39 g cm −3 ( x = 0) to 5.51 g cm −3 ( x = 0.06): afterwards, their values presented a downward trend, reducing to 4.01 g cm −3 at x = 0.48. Magnetic behaviors such as saturation magnetization ( ) and induction magnetization ( ) degraded as well as the real permeability of the samples by increasing the x content. The loss factor i.e. hysteresis loss also remarkably decreased by accumulation of SiO 2 and CaO in the grain boundaries. The electrical resistivity was determined in the order of 6.9 × 10 10 Ω cm for x = 0 and 6.4 × 10 11 Ω cm for x = 0.48. Therefore, low relative loss factor and high resistivity make these ferrites particularly useful as inductor and transformer materials for high frequency applications.

This publication has 21 references indexed in Scilit: