Abstract
Electrical, microstructural, and surface roughness of 150 nm sputtered pure samarium metal film on silicon substrates which thermal oxidized in oxygen ambient at various temperatures (600-900 °C) for 15 min have been investigated quantitatively. Effects of oxidation temperatures on the C-V characteristics, surface morphology, and surface roughness of Sm 2 O 3 thin films were reported. The smooth and uniform of Sm 2 O 3 thin films were revealed by scanning electron microscope and atomic force microscopy analysis. The sample oxidized at 700 °C demonstrated the smallest AV PB value, lowest STD value (5.56 × 10 12 cm -2 ) and D it values (~10 14 eV -1 cm -2 ).