Orthodontic Bracket Removal and Enamel Roughness: Comparing the Effects of Sapphire and Metallic Brackets in an In Vitro Study
Authors:
- Cosmin Bogdan LicsăndroiuCLCosmin Bogdan Licsăndroiu
- Mihaela Jana ȚuculinăMȚMihaela Jana Țuculină
- Adelina Smaranda BugălăABAdelina Smaranda Bugălă
- Petre Costin MărășescuPMPetre Costin Mărășescu
- Felicia Ileana MărășescuFMFelicia Ileana Mărășescu
- Andreea Gabriela NicolaANAndreea Gabriela Nicola
- Cristian Niky CumpătăCCCristian Niky Cumpătă
- Cosmin Mihai MirițoiuCMCosmin Mihai Mirițoiu
- Ovidiu Ioan GheorgheOGOvidiu Ioan Gheorghe
- Maria Cristina BeznaMBMaria Cristina Bezna
- Elena Verona LicsăndroiuELElena Verona Licsăndroiu
- Ionela Teodora DascăluIDIonela Teodora Dascălu
Open Access
- 28 September 2025
- journal article
- research article
- Published by MDPI AG in Bioengineering
- Vol. 12 (10) , 1041
Abstract
Background: Enamel surface roughness after bracket debonding is an important issue due to its impact on plaque accumulation and the potential development of carious lesions. This in vitro study aimed to assess enamel roughness after the removal of metallic and sapphire brackets and the effect of a remineralization treatment. Methods: Two hundred extracted human permanent teeth with healthy enamel were randomly distributed into two groups (n = 100) and bonded with either metallic or sapphire brackets using the same adhesive (3M™ Transbond™ XT (St. Paul, MN, USA), Minnesota Mining and Manufacturing Company, MN, USA). The enamel surface roughness was measured before bonding, after debonding, and after remineralization using SEM and a TR200 roughness (SaluTron GmbH, Frechen, Germany) tester. The parameter Ra was used to quantify the surface roughness. One-way ANOVA, the normality test, variance homogeneity, and the Bonferroni post hoc test were used to analyze the data. Results: Debonding significantly increased the enamel surface roughness in both groups. The sapphire bracket group presented significantly higher mean Ra values post debonding (4.14 ± 0.36 µm) compared to the metallic group (2.56 ± 0.52 µm). Remineralization led to a decrease in surface roughness in both groups, though not to baseline levels. The changes were statistically significant (p < 0.01), with a power of the test of 1.0. Conclusions: The bracket material significantly affects enamel surface roughness after orthodontic debonding. Sapphire brackets produced greater surface irregularities than metallic ones. Remineralization partially reduced roughness in both groups, with the final values in the metallic group being closer to baseline levels. Crucially, these values remained far above the clinical threshold for plaque retention, highlighting the need for improved debonding techniques.Keywords
Funding Information
- University of Medicine and Pharmacy of Craiova: Romania
This publication has 54 references indexed in Scilit:
- Biomimetic Construction of the Enamel-like Hierarchical StructureChemical Research in Chinese Universities, 2023
- Proximal enamel thickness of the permanent teeth: A systematic review and meta-analysisAmerican Journal of Orthodontics and Dentofacial Orthopedics, 2021
- In vitro evaluation of enamel surface roughness and morphology after orthodontic debonding: Traditional cleanup systems versus polymer burInternational Orthodontics, 2020
- Enamel demineralization around two different orthodontic bracket adhesive systems: An in vivo studyThe Saudi Dental Journal, 2019
- Gingival enlargement in orthodontic patients: Effect of treatment durationAmerican Journal of Orthodontics and Dentofacial Orthopedics, 2017
- Evaluation of enamel surface roughness after orthodontic bracket debonding with atomic force microscopyAmerican Journal of Orthodontics and Dentofacial Orthopedics, 2017
- Effect of simulated debracketing on enamel damageJournal of the Formosan Medical Association, 2012
- Effect of early orthodontic force on shear bond strength of orthodontic brackets bonded with different adhesive systemsAmerican Journal of Orthodontics and Dentofacial Orthopedics, 2010
- Surface roughness of the restored enamel after orthodontic treatmentAmerican Journal of Orthodontics and Dentofacial Orthopedics, 2010
- Evaluation of surface characteristics of dental composites using profilometry, scanning electron, atomic force microscopy and gloss-meterJournal of Materials Science: Materials in Medicine, 2007