SiC fiber strength after low pO 2 oxidation
- 28 September 2017
- journal article
- research article
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 101 (2) , 831-844
Abstract
Hi‐Nicalon™‐S SiC fiber was heat treated for 1 hour at 1300°C, 1400°C, and 1500°C in argon with pO 2 of 3.7, 10, 20, 50, 100, and 200 ppm. Fiber strengths were measured by 30 single‐filament tensile tests. Fiber microstructure and surface morphology were characterized by TEM . Active oxidation occurred in all cases except at 1500°C with 200 ppm pO 2 , 1400°C with 100 ppm pO 2 or higher, and 1300°C with 50 ppm pO 2 or higher. When active oxidation did not occur, a glass SiO 2 scale formed at 1300°C and 1400°C, and a cristobalite scale formed at 1500°C. The thickness of these scales was much larger than that predicted by linear dependence of oxidation rate on pO 2 . Fiber strengths were lowest after heat treatment at 1300°C and a pO 2 of 3.7 ppm, 1400°C and a pO 2 of 20 ppm, and 1500°C and a pO 2 of 200 ppm. Active oxidation caused fiber surface roughening, but no obvious changes to the internal fiber microstructure. Decreased fiber strength correlated with increased fiber surface roughness, but roughness magnitudes were not large enough to explain the amount by which strength was degraded. Fiber strengths, surface roughness, scale thicknesses, and the passive‐active oxidation transition for SiC are compared with previous observations. Possible strength degradation mechanisms are discussed.Keywords
This publication has 83 references indexed in Scilit:
- Processing, sintering and oxidation behavior of SiC fibers reinforced ZrB2 compositesJournal of the European Ceramic Society, 2012
- Pressure dependence of SiO2 growth kinetics and electrical properties on SiCJournal of Applied Physics, 2008
- Effect of heat treatment on the tensile strength and creep resistance of advanced SiC fibersJournal of Nuclear Materials, 2004
- Oxidation Kinetics and Mechanical Property of Stoichiometric SiC Fibers (Hi-Nicalon-S).Journal of the Ceramic Society of Japan, 2000
- Effect of Oxygen Partial Pressure on Oxidation Rate of Si-C-O FiberJournal of the Ceramic Society of Japan, 1998
- Preparation of Thin Sections of Coated Fibers for Characterization by Transmission Electron MicroscopyJournal of the American Ceramic Society, 1996
- SiO(g) formation from SiC in mixed oxidizing-reducing gasesOxidation of Metals, 1995
- Influence of Alumina Reaction Tube Impurities on the Oxidation of Chemically‐Vapor‐Deposited Silicon CarbideJournal of the American Ceramic Society, 1995
- High-temperature oxidation of silicon carbide in simulated atmospheric re-entry conditionsJournal of Materials Science, 1992
- High-temperature kinetics of the oxidation and nitridation of pyrolytic silicon carbide in dissociated gasesThe Journal of Physical Chemistry, 1970