Diffusion of manganese in cobalt and cobalt-manganese alloys

Authors:

Abstract
The diffusivities of manganese in cobalt and cobalt-manganese alloys have been determined by the residual-activity method with radioactive tracer Mn54 in the temperature ranges 860° to 1246°C in cobalt, 868° to 1200°C in Co-5·22 at. % Mn alloy, and 903° to 1148°C in Co-10·24 at. % Mn alloy. The observed effect of the magnetic transformation on the diffusion of manganese in cobalt and Co-5·22 at.% Mn alloy has been verified by examining the regression lines of the Arrhenius plots in the ferro- and paramagnetic phases. Arrhenius equations for the temperature dependence of diffusion coefficients are as follows: (1) in the ferromagnetic phase of cobalt, D = 3·15 × 10−2 exp [-(55 500 ± 1200)/RT]cm2/sec; (2) in the paramagnetic phase of cobalt, D = 1·10 × 10−2 exp [-(52 000 ± 4200)/RT]cm2/sec; (3) in the ferromagnetic phase of Co-5·22 at. % Mn alloy, D = 1·38 exp [-(64 100 ± 1500)/RT]cm2/sec; (4) in the paramagnetic phase of Co-5·22 at. % Mn alloy, D = 5·01 × 10−1 exp [-(61 300 ± 2400)/RT]cm2/sec; and (5) in the paramagnetic phase of Co-10·24 at. % Mn alloy, D = 1·36 exp [-(62 900 ± 810)/RT]cm2/sec. The difference in activation energies for impurity diffusion of the 3d-transition metals and self-diffusion in cobalt has been calculated using Le Claire's model and very good agreement with the experimental results has been obtained. The order of magnitude of the diffusivities of manganese in the iron group metals has been found to correspond with that of the self-diffusivities of these metals, namely D Mn/Ni > D Mn/Co > D Mn/γ-Fe and D N1/Ni > D Co/Co > D Fe/γ-Fe.

This publication has 21 references indexed in Scilit: