Measurement of Cohesion and Adhesion of Semiconducting Polymers by Scratch Testing: Effect of Side-Chain Length and Degree of Polymerization
- 1 August 2018
- journal article
- research article
- Published by American Chemical Society (ACS) in ACS Macro Letters
- Vol. 7 (8) , 1003-1009
Abstract
Most advantages of organic electronic materials are enabled by mechanical deformability, as flexible (and stretchable) devices made from these materials must be able to withstand roll-to-roll printing and survive mechanical insults from the external environment. Cohesion and adhesion are two properties that dictate the mechanical reliability of a flexible organic electronic device. In this paper, progressive-load scratch tests are used for the first time to correlate the cohesive and adhesive behavior of poly(3-alkylthiophenes) (P3ATs) with respect to two molecular parameters: length of the alkyl side chain and molecular weight. In contrast to metrological techniques based on buckling or pull testing of pseudofreestanding films, scratch tests reveal information about both the cohesive and adhesive properties of thin polymeric films from a single procedure. Our data show a decrease in cohesion and adhesion, that is, a decrease in overall mechanical robustness, with increasing length of the side chain. This behavior is likely due to increases in free volume and concomitant decreases in the glass transition temperature. In contrast, we observe increases in both the cohesion and adhesion with increasing molecular weight. This behavior is attributed to an increased density of entanglements with high molecular weight, which manifests as increased extensibility. These observations are consistent with the results of molecular dynamics simulations. Interestingly, the normal (applied) forces associated with cohesive and adhesive failure are directly proportional to the average degree of polymerization, as opposed to simply the molecular weight, as the length of the alkyl side chain increases the molecular weight without increasing the degree of polymerization.Keywords
Funding Information
- Air Force Office of Scientific Research (FA9550-16-1-0220)
- Division of Graduate Education (DGE-1144086)
This publication has 37 references indexed in Scilit:
- Mechanical Properties of Organic Semiconductors for Stretchable, Highly Flexible, and Mechanically Robust ElectronicsChemical Reviews, 2017
- Highly Efficient Organic Solar Cells Consisting of Double Bulk Heterojunction LayersAdvanced Materials, 2017
- Fully Printed Electrodes on Stretchable Textiles for Long‐Term ElectrophysiologyAdvanced Materials Technologies, 2017
- Intrinsically stretchable and healable semiconducting polymer for organic transistorsNature, 2016
- In situ vapor-deposited parylene substrates for ultra-thin, lightweight organic solar cellsOrganic Electronics, 2016
- Flexible, highly efficient all-polymer solar cellsNature Communications, 2015
- Thin film field-effect transistors of 2,6-diphenyl anthracene (DPA)Chemical Communications, 2015
- Stretchable, Transparent, Ultrasensitive, and Patchable Strain Sensor for Human–Machine Interfaces Comprising a Nanohybrid of Carbon Nanotubes and Conductive ElastomersACS Nano, 2015
- Transparent and Stretchable Interactive Human Machine Interface Based on Patterned Graphene HeterostructuresAdvanced Functional Materials, 2014
- An ultra-lightweight design for imperceptible plastic electronicsNature, 2013