Combustion Synthesis of TiB2-TiC Ceramic
Authors:
- 30 August 2013
- journal article
- Published by Trans Tech Publications, Ltd. in Applied Mechanics and Materials
- Vol. 380-384, 4323-4326
Abstract
TiB2-TiC multiphase ceramics were prepared through altering the molar ratio of Mg and C and leached with suitable acid by the combustion synthesis reaction of Mg, C, TiO2 and B2O3. The samples were investigated by XRD and SEM, and the results showed the diameter of the TiB2 was 1.5μm and the shape of the TiC was irregular spherical particles. The diameter and the proportion of the TiB2 were increased with the increase of Mg powder. The formation mechanism of TiB2 has been studied. The optimized proportioning of the molar ratio of Mg and C was 3:2.Keywords
This publication has 7 references indexed in Scilit:
- Low-temperature densification of TiB2 ceramic by the spark plasma sintering process with Ti as a sintering aidScripta Materialia, 2012
- Microstructure evolution and wear properties of in situ synthesized TiB2 and TiC reinforced steel matrix compositesJournal of Alloys and Compounds, 2008
- Titanium Diboride Thin Films by Low-Temperature Chemical Vapor Deposition from the Single Source Precursor Ti(BH4)3(1,2-dimethoxyethane)Chemistry of Materials, 2007
- Effect of HCl concentration on TiB2 separation from a self-propagating high-temperature synthesis (SHS) productMaterials Research Bulletin, 2007
- Preparation of TiB2 powders by mechanical alloyingMaterials Letters, 2002
- Mechanical enhancement of the carbothermic formation of TiB2Metallurgical and Materials Transactions A, 2000
- TiC + TiB2 composite shows wear promiseMetal Powder Report, 1997