Fluoride-containing nanoporous calcium-silicate MTA cements for endodontics and oral surgery: early fluorapatite formation in a phosphate-containing solution
- 5 July 2011
- journal article
- Published by Wiley in International Endodontic Journal
- Vol. 44 (10) , 938-949
Abstract
Gandolfi MG, Taddei P, Siboni F, Modena E, Ginebra MP, Prati C. Fluoride-containing nanoporous calcium-silicate MTA cements for endodontics and oral surgery: early fluorapatite formation in a phosphate-containing solution. International Endodontic Journal, 44, 938–949, 2011. Abstract Aim To test the chemical–physical properties and apatite-forming ability of experimental fluoride-doped calcium silicate cements designed to create novel bioactive materials for use in endodontics and oral surgery. Methodology A thermally treated calcium silicate cement (wTC) containing CaCl2 5%wt was modified by adding NaF 1%wt (FTC) or 10%wt (F10TC). Cements were analysed by environmental scanning electron microscopy with energy-dispersive X-ray analysis, IR and micro-Raman spectroscopy in wet conditions immediately after preparation or after ageing in a phosphate-containing solution (Dulbecco’s phosphate-buffered saline). Calcium and fluoride release and pH of the storage solution were measured. The results obtained were analysed statistically (Tukey’s HSD test and two-way anova). Results The formation of calcium phosphate precipitates (spherulites) was observed on the surface of 24 h-aged cements and the formation of a thick bone-like B-type carbonated apatite layer (biocoating) on 28 day-aged cements. The rate of apatite formation was FTC > F10TC > wTC. Fluorapatite was detected on FTC and F10TC after 1 day of ageing, with a higher fluoride content on F10TC. All the cements released calcium ions. At 5 and 24 h, the wTC had the significantly highest calcium release (P < 0.001) that decreased significantly over the storage time. At 3–28 days, FTC and F10TC had significantly higher calcium release than wTC (P < 0.05). The F10TC had the significantly highest fluoride release at all times (P < 0.01) that decreased significantly over storage time. No significant differences were observed between FTC and wTC. All the cements had a strong alkalinizing activity (OH− release) that remained after 28 days of storage. Conclusions The addition of sodium fluoride accelerated apatite formation on calcium silicate cements. Fluoride-doped calcium silicate cements had higher bioactivity and earlier formation of fluorapatite. Sodium fluoride may be introduced in the formulation of mineral trioxide aggregate cements to enhance their biological behaviour. F-doped calcium silicate cements are promising bone cements for clinical endodontic use.Keywords
This publication has 36 references indexed in Scilit:
- Biological responses of human osteoblasts and osteoclasts to flame-sprayed coatings of hydroxyapatite and fluorapatite blendsActa Biomaterialia, 2010
- Solubility in water or DMEM of F-doped MTA cements with increasing F-contentDental Materials, 2010
- Setting time and expansion in different soaking media of experimental accelerated calcium-silicate cements and ProRoot MTAOral Surgery Oral Medicine Oral Pathology Oral Radiology and Endodontology, 2009
- Kinetics of apatite formation on a calcium-silicate cement for root-end filling during ageing in physiological-like phosphate solutionsClinical Oral Investigations, 2009
- Controlled Release Scaffolds for Bone Tissue EngineeringJournal of Pharmaceutical Sciences, 2009
- Calcium silicate coating derived from Portland cement as treatment for hypersensitive dentineJournal of Dentistry, 2008
- Fluoride-Containing Bioactive GlassesAdvanced Materials Research, 2008
- New Portland Cement–based Materials for Endodontics Mixed with Articaine Solution: A Study of Cellular ResponseJournal of Endodontics, 2008
- An evaluation of accelerated Portland cement as a restorative materialBiomaterials, 2002
- The Fluoridation of Nonstoichiometric Calcium Hydroxyapatite. An Infrared StudyCanadian Journal of Chemistry, 1974