The present report represents, physicochemical characteristics of pure and Mn4+ substituted SnO2 nanocrystals [Sn(1-x)MnxO2 NCs, where x = 0, 0.05, and 0.10], synthesized using the co-precipitation technique. Structural characterization revealed that all the compositions possessed tetragonal crystal phase with space group P4/2mnm with no signature of impurities. Microstructural characterization depicted that the average grain size decreased from 34 nm to 22 nm with Mn4+ doping in the host SnO2. The appearance of 643 cm-1 and 484 cm-1 attributes to O-Sn-O and Sn-O vibrations, which confirmed the formation of Sn(1-x)MnxO2 NCs. The electrical characterizations were conducted using Hall effect measurements and it was observed that doping of Mn4+ in the crystal framework of host SnO2 decreases the carrier concentration (n) from 5.73 × 1016 cm-3 to 3.36 × 1016 cm-3 whereas the mobility (μ) decreases from 5.18 cm2/Vs to 2.35 cm2/Vs thereby transforming the system from n-type behavior of pristine SnO2 to p-type with Mn4+ doping. The dielectric constant also decreases with increasing Mn4+ concentration in the system. I-V characteristics show linear behavior with improved resistance with the addition of Mn4+ to SnO2.