Ball-Milling Processing of Hydrogenated NdFeB Powders from the Recycling of End-of-Life Magnets
Authors:
- Amanuel Elias WakoAWAmanuel Elias Wako
- Pablo RodríguezPRPablo Rodríguez
- Beatrice MuzziBMBeatrice Muzzi
- Giovanna TrevisiGTGiovanna Trevisi
- Laura GrauLGLaura Grau
- Martin AlbinoMAMartin Albino
- Tomaž TomšeTTTomaž Tomše
- Benjamin PodmiljsakBPBenjamin Podmiljsak
- Carlo BurkhardtCBCarlo Burkhardt
- Franca AlbertiniFAFranca Albertini
- Claudio SangregorioCSClaudio Sangregorio
- César de Julián FernándezCésar de Julián Fernández
Open Access
- 6 September 2026
- Vol. 19 (17) , 3797
Abstract
Rare-earth-based permanent magnets are key elements for today’s technologies. Their recycling is crucial for securing the supply of critical raw materials and ensuring a sustainable circular economy in magnet production. In this study, hydrogen decrepitated NdFeB powders recovered from end-of-life magnets were processed using planetary ball milling to obtain powders suitable for recycled magnet production. The magnets were sourced from a wind turbine, scooter motor, and ring magnet, and exhibit different compositions and properties. The structural, morphological, and magnetic properties of the hydrogenated and ball-milled powders were investigated considering the effects of the milling time and ball diameters. Submicron-sized powders were achieved within 10 min with 5 mm balls, while longer milling times were required to obtain similar particle size reduction with 10 mm balls. Milling resulted in structural damage to the hydrogenated powders. Furthermore, although milling decreased the magnetization of the powders, an increase in the coercive field was observed for certain milling times. Micrometric powders sourced from the wind turbine, milled for 10 min using 5 mm balls, exhibited the highest coercive field of 0.27 T. This behavior is discussed considering the effect of the particle size reduction, the structural damage, the particle agglomeration, and the local compositional changes. We conclude that the powders produced from different source magnets exhibit similar patterns of morphological, structural, and magnetic changes under milling, and only the Tc and the Hc of the powders depend on their original magnet. Ball milling represents a promising technique for particle size refining in the hydrogen processing of magnetic scraps, a crucial step in the magnet-to-magnet recycling process.Keywords
Funding Information
- European Institute of Innovation and Technology (EIT) Raw Materials (20090)
- European Commission (101129888)
This publication has 47 references indexed in Scilit:
- The current status of recycling technology for waste NdFeB resourcesJournal of Material Cycles and Waste Management, 2025
- Microstructural Investigation of Discarded NdFeB Magnets After Low-Temperature HydrogenationJournal of Sustainable Metallurgy, 2024
- Towards an Alloy Recycling of Nd–Fe–B Permanent Magnets in a Circular EconomyJournal of Sustainable Metallurgy, 2018
- Characterization of Polycrystalline Fe2B Compound with High Saturation MagnetizationJournal of Superconductivity and Novel Magnetism, 2017
- Recycling of scrap sintered Nd–Fe–B magnets as anisotropic bonded magnets via hydrogen decrepitation processJournal of Material Cycles and Waste Management, 2014
- Magnetic Materials and Devices for the 21st Century: Stronger, Lighter, and More Energy EfficientAdvanced Materials, 2010
- Effect of hydrogen on the magnetic characteristicsof Nd2Fe14B single crystalPhysica Status Solidi (a), 2003
- A study of Nd-Fe-B magnets produced using a combination of hydrogen decrepitation and jet millingJournal of Materials Science, 1989
- Effects of hydrogen absorption on the 3d and 4f anisotropies in RE2Fe14B (RE ≡ Y, Nd, Ho, Tm)Journal of the Less Common Metals, 1988
- Theory of Nucleation Fields in Inhomogeneous FerromagnetsPhysica Status Solidi (b), 1987