The effect of phase on microstructure and mechanical performance in TiAlN and TiSiN films
Authors:
- Lili DuanLDLili Duan
- Hua WuHWHua Wu
- Liming GuoLGLiming Guo
- Wencui XiuWXWencui Xiu
- Xiaofeng YuXYXiaofeng Yu
Open Access
- 1 June 2020
- journal article
- research article
- Published by IOP Publishing in Materials Research Express
- Vol. 7 (6) , 066401
Abstract
To study the effect of phase on the microstructure and mechanical properties of nitride coatings, three films of TiN, TiAlN, and TiSiN were prepared on the surface of high-speed steel using hollow cathode assisted multi-arc ion plating technique. The XRD lines of the three films were analyzed and calculated by linear analysis. The element and phase of the film were observed and analyzed by x-ray Diffraction (XRD), Transmission Electron Microscope (TEM), energy dispersive x-ray analysis (EDS). The microstructure and film thickness of the coating were characterized by scanning electron microscopy (SEM). The surface roughness of the film was observed by Confocal laser scanning microscope (CLSM). The hardness, friction coefficient, and coating/substrate adhesion of the film were tested by the G200 nanometer hardness tester and CETR UNMT-1 surface micro-nano mechanical test system. We discovered two different reinforcement mechanisms. The high microscopic strain value (1.309 × 10−3) in the TiAlN film was related to the formation of Ti3AlN substitutional solid solution in the film formed a large lattice distortion,however, the coating/substrate adhesion (33.5 N) was lowered. The result of independent nucleation and growth of the Si3N4 phase in the TiSiN film refines the structure of the film, alleviating the increase of microscopic strain. At this time, the coating/substrate adhesion reaches the highest value of 40 N and the film surface roughness reaches the minimum value of 0.451 μm. The results also show that the TiSiN coating can obtain good coating/substrate adhesion without pre-plating.Keywords
This publication has 29 references indexed in Scilit:
- Tribological and mechanical properties of multilayered TiVN/TiSiN coatings synthesized by cathodic arc evaporationSurface and Coatings Technology, 2018
- Frictional and wear performance of TiAlN/TiN coated tool against high-strength steelCeramics International, 2018
- Improving thermal stability of TiSiN nanocomposite coatings by multilayered epitaxial growthSurface and Coatings Technology, 2017
- Influence of TiN-nanolayered insertions on microstructure and mechanical properties of TiSiN nanocomposite filmJournal of Materials Science, 2014
- Effect of silicon content on PVD film mechanical properties and cutting performance of coated cemented carbide insertsSurface and Coatings Technology, 2013
- Wear mechanisms of PVD-coated PCBN cutting toolsWear, 2013
- Approximation of crystallite size and microstrain via XRD line broadening analysis in TiSiN thin filmsVacuum, 2012
- Optimization of the Adhesion Strength of Arc Ion Plating TiAlN Films by the Taguchi MethodMaterials, 2009
- Stress and preferred orientation in nitride-based PVD coatingsSurface and Coatings Technology, 2008
- INTRODUCTION TO RESIDUAL STRESS1987