Abstract
This paper presents a study of hydrogen diffusion for a spiral weld pipe considering the effect of weld residual stress. The results show that the hydrogen mainly gathers at heat-affected zone (HAZ). HAZ is the weakest zone where hydrogen-induced cracking (HIC) occurs. The effect of helix angle on the hydrogen diffusion is also discussed. It shows that different helix angles generate different hydrogen concentrations. As the helix angle increases, both the hydrogen concentration and residual stresses decrease. As the helix angle increases from 40 deg to 50 deg, the equivalent pressure stresses reduce a little, resulting in the change of hydrogen concentration being small. The smaller the helix angle is, the larger the diffusion rate is. The most suitable helix angle should be optimized at 40–50 deg.Keywords
Funding Information
- National Natural Science Foundation of China (11372359 and 515755)
This publication has 39 references indexed in Scilit:
- 3D cohesive modelling of hydrogen embrittlement in the heat affected zone of an X70 pipeline steelInternational Journal of Hydrogen Energy, 2013
- Hydrogen diffusion and hydrogen influenced critical stress intensity in an API X70 pipeline steel welded joint – Experiments and FE simulationsInternational Journal of Hydrogen Energy, 2012
- Residual stress prediction in submerged arc welded spiral pipesMaterials & Design (1980-2015), 2012
- Evaluation of threshold stress intensity factor of hydrogen embrittlement cracking by indentation testingMaterials Science and Engineering: A, 2012
- Residual stress measurement of new and in-service X70 pipelines by X-ray diffraction methodNDT & E International, 2011
- Thermal stress analysis of spiral laser-welded tubeJournal of Materials Processing Technology, 2011
- Analysis of electrochemical hydrogen permeation through X-65 pipeline steel and its implications on pipeline stress corrosion crackingInternational Journal of Hydrogen Energy, 2007
- Comparison on the cracking susceptibility of different low alloy steel weldments exposed to the environment containing wet H2SEngineering Failure Analysis, 2006
- Hydrogen interaction and stress-corrosion in hydrocarbon storage vessel and pipeline weldingsInternational Journal of Hydrogen Energy, 2006
- Analysis of temperature and stress field in Al alloy’s twin wire weldingTheoretical and Applied Fracture Mechanics, 2005