Phase Transformation and Properties of Fe-Cr-Co Alloys with Low Cobalt Content
Authors:
- 1 January 2015
- journal article
- Published by Japan Institute of Metals in MATERIALS TRANSACTIONS
- Vol. 56 (9) , 1491-1495
Abstract
No abstract availableThis publication has 31 references indexed in Scilit:
- Gradient Microstructure of FeCr30Co8 Hard Magnetic Alloy Subjected to Plastic Deformation by Tension Combined with Torsion at 700 and 720°CSolid State Phenomena, 2012
- Effect of Cr content on the thermal stability of tempered lath structures and precipitates in strength enhanced ferritic steelsJournal of Physics: Conference Series, 2010
- Structural studies, magnetic properties and loss separation in iron–phenolicsilane soft magnetic compositesMaterials & Design (1980-2015), 2010
- Deformation texture and magnetic properties of dual-phase Fe–Co–V alloysMaterials & Design (1980-2015), 2009
- Magnetic domain structures in Co–Ni–Al shape memory alloys studied by Lorentz microscopy and electron holographyActa Materialia, 2002
- Ab initiocalculations of exchange interactions, spin-wave stiffness constants, and Curie temperatures of Fe, Co, and NiPhysical Review B, 2001
- Microhardness and microstructure of austenite and ferrite in nitrogen alloyed duplex steels between 20 and 500°CMaterials Science and Engineering: A, 1998
- Oscillations in exchange coupling and magnetoresistance in metallic superlattice structures: Co/Ru, Co/Cr, and Fe/CrPhysical Review Letters, 1990
- Phase diagram of Fe-Cr-Co permanent magnet systemIEEE Transactions on Magnetics, 1977
- Fe-Cr-Co permanent magnet alloys containing Nb and AlIEEE Transactions on Magnetics, 1975