Abstract
Metal-assisted silicon etching in the HF/H2O2/H2O solution with silver ions as a catalyst was investigated. It is found that geometric parameters of layers of nanostructured silicon are determined by the silver-catalyst concentration. A spontaneous stop of the etching process at low Ag+ ion concentration is explained by formation of insoluble Ag2SiO3.Keywords
This publication has 11 references indexed in Scilit:
- Ag-Mediated Charge Transport during Metal-Assisted Chemical Etching of Silicon NanowiresACS Applied Materials & Interfaces, 2013
- Effect of etching time on morphological, optical, and electronic properties of silicon nanowiresDiscover Nano, 2012
- Metal assisted chemical etching for high aspect ratio nanostructures: A review of characteristics and applications in photovoltaicsCurrent Opinion in Solid State and Materials Science, 2012
- Metal‐Assisted Chemical Etching of Silicon: A ReviewAdvanced Materials, 2010
- Localisation of silicon nanowires grown by UHV-CVD in (111)-oriented apertures opened in Si (001)IOP Conference Series: Materials Science and Engineering, 2009
- Pore formation in silicon by wet etching using micrometre-sized metal particles as catalystsJournal of Materials Chemistry, 2008
- Facile Method To Fabricate a Large-Scale Superhydrophobic Surface by Galvanic Cell ReactionChemistry of Materials, 2006
- SU8 photoresist as an etch mask for local deep anodic etching of siliconPhysica Status Solidi (a), 2003
- Quasi-one-dimensional distribution of macropores in anodically etched uniaxially stressed silicon platesTechnical Physics Letters, 2003
- Openings in Photoelectrochemistry and Photocorrosion of SiliconZeitschrift für Physikalische Chemie, 1999