Abstract
In this paper, the effect of TiN capping layer on interface quality and the channel hot carrier (CHC) reliability of high-k/metal-gate (HKMG) nMOSFET was investigated. Experiments show that the fresh interface trap density was reduced from 1.83×1011 cm-2 to 7.75×1010 cm-2 for 1.4nm and 2.4nm ALD TiN capping layers respectively, while the CHC time-to-failure was worsened by 13%. Combining the chemical analysis by secondary ion mass spectroscopy and the characterization of active energy for trap generation, it’s found that the extraordinary chlorine introduced by ALD TiN capping layer deposition could be responsible for the improved fresh interfacial trap but degraded CHC reliability in HKMG nMOSFETs. The mechanism can be explained by the lower binding energy of Si-Cl than Si-H, which results in more interface passivation but easier to be broken by electrical stress. This finding can provide the guide for the optimization of HKMG process.
Funding Information
  • National High Technology Research and Development Program 863 (2015AA016501)
  • National Natural Science Foundation of China (61306129)

This publication has 13 references indexed in Scilit: