In‐vitro Degradation and Bioactivity of Tailored Amorphous Multi Porous Scaffold Structure
- 24 February 2012
- journal article
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 95 (9) , 2687-2694
Abstract
A key requirement for the use of bio scaffold is that its degradation rate matches the growth rate of target tissue. Therefore, the degradation of recently developed tailored amorphous multiporous ( TAMP ) scaffold of 70 SiO 2 ·30 CaO (mol%) in simulated body fluid ( SBF ) was studied under both static and quasi‐dynamic conditions. The degradation was assessed through the dissolution of silica from the glass into SBF , while the in‐vitro bioactivity was characterized by precipitation of calcium phosphate ( CaP ) on and inside the scaffold. Under static conditions, the degradation stopped due to the saturation of solution with silica in 3 days, whereas the precipitation of CaP continued. Rapid degradation and better in‐vitro bioactivity was found under quasi‐dynamic conditions, where the concentration gradient across the sample was maintained. The degradation followed exponential dependence on time with a half‐life of 15.4 days and initial degradation rate 4.5% day −1 . The remaining samples maintained their integrity and pore structure during degradation. The degradation occurred in three distinct stages: (a) wetting stage, (b) initial degradation stage when CaP precipitation dominates, and (c) intensive degradation stage when the nanopores rupture and network dissolves. By varying the sintering parameters the nanopore structure, and hence the degradation rate, can be tailored to suit the anticipated tissue regeneration rate. With demonstrated rapid and controllable degradation and good in‐vitro bioactivity, the TAMP scaffold shows promise as candidate for bone regeneration application under various conditions in the body.Keywords
This publication has 24 references indexed in Scilit:
- Melt-derived bioactive glass scaffolds produced by a gel-cast foaming techniqueActa Biomaterialia, 2011
- Oriented bioactive glass (13-93) scaffolds with controllable pore size by unidirectional freezing of camphene-based suspensions: Microstructure and mechanical responseActa Biomaterialia, 2011
- High Surface Area Nanomacroporous Bioactive Glass Scaffold for Hard Tissue EngineeringJournal of the American Ceramic Society, 2010
- Growth and differentiation of osteoblastic cells on 13–93 bioactive glass fibers and scaffoldsActa Biomaterialia, 2008
- Extracellular matrix formation and mineralization on a phosphate-free porous bioactive glass scaffold using primary human osteoblast (HOB) cellsBiomaterials, 2007
- Resorbable, porous glass scaffolds by a salt sintering processJournal of Materials Science, 2006
- 45S5 Bioglass®-derived glass–ceramic scaffolds for bone tissue engineeringBiomaterials, 2006
- Optimising bioactive glass scaffolds for bone tissue engineeringBiomaterials, 2006
- Cellular materials as porous scaffolds for tissue engineeringProgress in Materials Science, 2001
- Effect of Texture on the Rate of Hydroxyapatite Formation on Gel‐Silica SurfaceJournal of the American Ceramic Society, 1995