Influence of Enamel Thickness on Quantification of Mineral Loss in Enamel Using Laser-Induced Fluorescence

Authors:
  • BSB.R. Schemehorn
    B.R. Schemehorn
  • GEG.J. Eckert
    G.J. Eckert
  • DZD.T. Zero
    D.T. Zero
  • GSG.K. Stookey
    G.K. Stookey

Abstract
The objective of this study was to evaluate the effect of enamel thickness on the quantification of white-spot lesions with laser fluorescence. One hundred and twenty 3-mm-diameter human ground and polished enamel specimens were used. Specimens were illuminated by a 488-nm argon laser, images were acquired through a 540-nm high-pass filter and stored on the Quantitative Light-Induced Fluorescence (QLF) program. Specimens were divided into two groups and demineralized for 48 or 96 h and QLF images were again acquired. Fluorescence radiance (FR) of both sound (FRs) and demineralized (FRd) enamel was determined using the QLF program. Change in fluorescence radiance (ΔFR, %) was determined as follows: ΔFR = FRd/FRs × 100. One thin section was obtained for transverse microradiography analysis. Enamel and dentin thickness of the thin sections were measured. There was a good correlation between QLF parameters and enamel thickness. It can be concluded that the FR observed for similar lesions depends on the actual enamel thickness.