Phase Equilibria in Co-Rich Co-Al-W Alloys at 1300°C and 900°C
Authors:
- 7 June 2011
- journal article
- Published by Trans Tech Publications, Ltd. in Materials Science Forum
- Vol. 686, 388-391
Abstract
The phase equilibria of Co-base trial alloys of Co-9Al-7.5W, Co-5.5Al-10W and Co-9Al-3W at 1300°C and 900°C were determined in the present investigation. The experimental alloys were γ single-phase alloys at 1300°C, although the existence of the γ' phase and the ε phase was identified due to cooling effect. The nearly cuboidal γ' phase and the plate-like DO19 phase in alloys 9Al-7.5W and 5.5Al-10W were coarsened after long-term annealing at 900°C. It is suggested that the alloy 9Al-7.5W was in γ+γ' two-phase region, while the alloys 5.5Al-10W and 9Al-3W were in γ+DO19 two-phase region and γ singe-phase region at 900°C, respectively.Keywords
This publication has 7 references indexed in Scilit:
- Mo Effect on the Microstructure in Co-Al-W-Based SuperalloysMaterials Science Forum, 2010
- New Co-based γ-γ′ high-temperature alloysJOM, 2010
- Determination of phase equilibria in the Co-rich Co–Al–W ternary system with a diffusion-couple techniqueIntermetallics, 2009
- High-temperature strength and deformation of γ/γ′ two-phase Co–Al–W-base alloysActa Materialia, 2008
- Flow stress anomalies in γ/γ′ two-phase Co–Al–W-base alloysScripta Materialia, 2007
- Mechanical Properties of Co-Based L12 Intermetallic Compound Co3(Al,W)MATERIALS TRANSACTIONS, 2007
- Cobalt-Base High-Temperature AlloysScience, 2006