Properties of chemical bath deposited and sensitized PbSe thin films for IR detection

Authors:

Abstract
PbSe thin films of one-micron thickness were deposited on SiO 2 /Si wafers using chemical bath deposition method for IR detector applications. To sensitize the PbSe films for efficient mid-wave IR detection in the spectral range from 3 to 5 μ m, oxidation at 460 °C and subsequent iodization at 350 °C were performed. The x-ray diffraction for as-grown PbSe shows poly-crystalline face-centered cubic NaCl type structure while Pb 3 O 2 (SeO 3 ) oxide peak develops as a function of oxidation time. The existence of Se-rich structure may lead to p -type conduction. Scanning electron microscope and cross-sectional energy dispersive x-ray depth profile measurements after oxidation show the top layer of the film contains primarily Pb-Se-oxide while film at the bottom layer was PbSe. After sensitization, polytype trigonal 12R PbI 2 , Pb 3 O 2 I 2 and PbSe were confirmed. The top layer of the sensitized PbSe film was found to be converted to primarily PbI 2 while the bottom layer remained PbSe. However, during sensitization without oxidation, little PbSe remained because most of the PbSe was converted into PbI 2 . Also, the presence of metallic Pb nano-crystals with 10 nm diameter was detected in the sensitized film.
Funding Information
  • Defense Advanced Research Projects Agency (FA8650-16-C-7637)

This publication has 50 references indexed in Scilit: