On the structure of Ni–Cr–B–Si hardfacing alloys and their bonding reactions

Authors:

Abstract
Silicon is dissolved in the nickel-rich mixed crystal of Ni–Cr–B–Si alloys which are used for hardfacing. Boron forms several different borides due to the small solubility in the mixed crystals. There is a wide liquidus range during solidification of these alloys caused by the metastable solidification of the Ni–Ni2B eutectic instead of the stable solidification of the Ni–Ni3B eutectic. This wide liquidus range facilitates the hardfacing process which can be conveniently done by fusing the alloyed powders in a furnace. The hot hardness of nickel-based hard alloys is higher, up to 900 °C. The boron diffusion into the base metal is of the volume diffusion type; no grain boundary diffusion was observed with type 316 stainless steel.