The influence of slag chemistry on the formation of sliver defects
Authors:
- 26 November 2017
- journal article
- research article
- Published by SAGE Publications in Ironmaking & Steelmaking: Processes, Products and Applications
- Vol. 46 (5) , 463-468
Abstract
The reoxidation of molten steel by oxidising slag directly affects the molten steel cleanliness. There is a good relationship between molten steel cleanliness and the defect sources of cold rolled sheets. The results show that there is a direct relationship of the slag composition to steel cleanliness and the rate of surface defects on the final products. The thermodynamic calculations show that the activity of iron oxide decreases with the increase of w(CaO)/w(Al2O3) specifically when the content of T.Fe in slag remains at lower levels. In order to enhance the absorption ability of the slag to Al2O3 inclusions, w(CaO)/w(Al2O3) should be controlled in the range of 1.0–1.4 in the liquid region of slag when T.Fe content in RH final slag is less than 6 mass%. By reasonable control of T.Fe content and w(CaO)/w(Al2O3) in the slag, the defect content of sheets significantly declines.Keywords
This publication has 4 references indexed in Scilit:
- Finite element simulation of flexible roll forming with supplemented material data and the experimental verificationChinese Journal of Mechanical Engineering, 2015
- The Ability of Slags to Absorb Solid Oxide InclusionsISIJ International, 2006
- Influence of Sulphur Content and Molten Steel Flow on Entrapment of Bubbles to Solid/Liquid InterfaceISIJ International, 2006
- Wetting of Solid Al2O3 with Molten CaO-Al2O3-SiO2ISIJ International, 2003