Assessment of Platinum Dissolution from a Pt/C Fuel Cell Catalyst: An Electrochemical Quartz Crystal Microbalance Study
- 1 January 2010
- journal article
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 157 (5) , B621-B627
Abstract
The stability of different types of platinum surfaces in the presence of chloride was evaluated by applying a potential of 1.2 V vs reversible hydrogen electrode while the associated mass change in the Pt electrode was monitored with an electrochemical quartz crystal microbalance. The platinum metal surfaces based on the particles and films show a large difference toward dissolution when exposed to small amounts of chloride. While an electrodeposited platinum metal film showed no degradation in a sulfuric acid solution containing 10 ppm of chloride, an electrode made from a fuel cell catalyst (50 wt % Pt/C) lost 10% of its platinum content over a 24 h period when exposed to a sulfuric acid solution containing 10 ppm of chloride. At a chloride concentration of 20 ppm, the onset potential of the Pt oxide formation increased ∼200mV∼200mV compared to an electrode in a chloride-free solution. The degradation of nanoparticles thus appears to be much more significant than for the electrodeposited platinum electrodes.Keywords
This publication has 36 references indexed in Scilit:
- Dissolution of platinum in acidic mediaElectrochimica Acta, 2008
- An investigation into factors affecting the stability of carbons and carbon supported platinum and platinum/cobalt alloy catalysts during 1.2V potentiostatic hold regimes at a range of temperaturesJournal of Power Sources, 2007
- A review of PEM hydrogen fuel cell contamination: Impacts, mechanisms, and mitigationJournal of Power Sources, 2007
- Stabilization of Platinum Oxygen-Reduction Electrocatalysts Using Gold ClustersScience, 2007
- Durability investigation of carbon nanotube as catalyst support for proton exchange membrane fuel cellJournal of Power Sources, 2006
- Anisotropic Dissolution of an Au(111) Electrode in Perchloric Acid Solution Containing Chloride Anion Investigated by in Situ STMThe Important Role of Adsorbed Chloride AnionLangmuir, 1998
- An In Situ Electrochemical Quartz Crystal Microbalance Study of the Dissolution Process of a Gold Electrode in Perchloric Acid Solution Containing Chloride IonJournal of the Electrochemical Society, 1998
- Crystallite growth of platinum dispersed on graphitized carbon black II. Effect of liquid environmentJournal of Catalysis, 1976
- A ring-disk electrode study of the current/potential behaviour of platinum in 1.0 M sulphuric and 0.1 M perchloric acidsElectrochimica Acta, 1970
- Emf Measurements on the System Platinum(IV)/Platinum(II) in a Chloride Ion Medium at 60 degrees C.Acta Chemica Scandinavica, 1968