Experimental Investigation of Effect of L-Profile Hybrid Aluminium/GFRP to the Axial and Lateral Characteristic
Authors:
- Ariyana Dwiputra NugrahaANAriyana Dwiputra Nugraha
- Daffa AlandroDADaffa Alandro
- Arif KusumawantoAKArif Kusumawanto
- Endro JuniantoEJEndro Junianto
- Budi PerwaraBPBudi Perwara
- Vishnu Vijay KumarVishnu Vijay Kumar
- Gil Nonato C. SantosGSGil Nonato C. Santos
- Jayan SentanuhadyJSJayan Sentanuhady
- Rachmadi NorcahyoRNRachmadi Norcahyo
- Muhammad Akhsin MuflikhunMuhammad Akhsin Muflikhun
Open Access
Abstract
The current study investigates the effect of a hybrid L-profile aluminium/glass-fiber-reinforced polymer stacking sequence under axial and lateral compression loads. Four stacking sequences are studied: aluminium (A)—glass-fiber (GF)—AGF, GFA, GFAGF, and AGFA. In the axial compression test, the aluminium/GFRP hybrid tends to crush in a more progressive and stable failure than the net aluminium and net GFRP specimens, with a relatively more stable load-carrying capacity throughout the experimental tests. The AGF stacking sequence was second, with an energy absorption of 145.31 kJ, following AGFA at 157.19 kJ. The load-carrying capacity of AGFA was the highest, with an average peak crushing force of 24.59 kN. The second-highest peak crushing force, 14.94 kN, was achieved by GFAGF. The highest amount of energy absorption, 157.19 J, was achieved by the AGFA specimen. The lateral compression test showed a significant increase in load-carrying and energy absorption capacity in the aluminium/GFRP hybrid specimens compared to the net GFRP specimens. AGF had the highest energy absorption with 10.41 J, followed by AGFA with 9.49 J. AGF also had the highest peak crushing force with 2.98 kN, followed by AGFA with 2.16 kN. The most crashworthy stacking sequence among the four variations tested in this experimental research was the AGF stacking sequence because of its great load-carrying capacity, energy absorption, and specific energy absorption in axial and lateral loading. The study provides greater insight into the failure of hybrid composite laminates under lateral and axial compression.Keywords
This publication has 31 references indexed in Scilit:
- Design for cost performance of crashworthy structures made of high strength steelThin-Walled Structures, 2019
- A Review of Recent Advances in Nanoengineered Polymer CompositesPolymers, 2019
- Electrospun nanofiber interleaving in fiber reinforced composites—Recent trendsMaterial Design & Processing Communications, 2018
- High-velocity impact behaviour of aluminium honeycomb sandwich panels with different structural configurationsInternational Journal of Impact Engineering, 2018
- Energy absorption of bio-inspired multi-cell CFRP and aluminum square tubesComposites Part B: Engineering, 2017
- Experimental study on crashworthiness of empty/aluminum foam/honeycomb-filled CFRP tubesComposite Structures, 2016
- Lightweight design and crash analysis of composite frontal impact energy absorbing structuresComposite Structures, 2012
- Composite steel–CFRP SHS tubes under axial impactComposite Structures, 2009
- On the response of thin-walled CFRP composite tubular components subjected to static and dynamic axial compressive loading: experimentalComposite Structures, 2005
- Dynamic axial crushing of combined composite aluminium tube: the role of both reinforcement and surface treatmentsComposite Structures, 2002