Adhesive bonding of a lithium disilicate ceramic material with resin‐based luting agents
Authors:
- 6 July 2005
- journal article
- Published by Wiley in Journal of Oral Rehabilitation
- Vol. 32 (8) , 598-605
Abstract
summary This study evaluates the bonding characteristics of a lithium disilicate‐based ceramic material (IPS Empress 2). Two sizes of disk specimens of the material were made, and three groups of disk pairs were separately surface‐prepared using three techniques; etching with phosphoric acid, etching with hydrofluoric acid, and air‐abrasion with alumina. Each group was further divided into four sub‐groups; group (i) was bonded with the Variolink II composite, (ii) was treated with the Monobond‐S silane primer and bonded with the Variolink II composite, (iii) was bonded with the Super‐Bond acrylic adhesive and (iv) was treated with the Porcelain Liner M silane primer and bonded with the Super‐Bond acrylic adhesive. Shear bond strengths were determined before and after 100 000 thermocycles. Bond strength varied from 10·6 to 71·5 MPa before thermocycling, whereas post‐thermocycling bond strength ranged from 0 to 61·2 MPa. Among the three surface preparations, hydrofluoric acid etching (HF) was most effective in enhancing bond strength of both luting materials, especially for unsilanized specimens. Application of the silane primer elevated bond strength of both luting agents regardless of surface preparation method. It can be concluded, for both luting agents, that durable bond to the Empress 2 ceramic material can be achieved through the combined application of HF and the proprietary silane primer.Keywords
This publication has 20 references indexed in Scilit:
- Effectiveness of two‐liquid silane primers on bonding sintered feldspathic porcelain with a dual‐cured composite luting agentJournal of Oral Rehabilitation, 2004
- Strength, fracture toughness and microstructure of a selection of all-ceramic materials. Part I. Pressable and alumina glass-infiltrated ceramicsDental Materials, 2004
- Evaluation of fracture resistance of endodontically treated maxillary premolars, restored with ceromer or heat‐pressed ceramic inlays and fixed with dual‐resin cementsJournal of Oral Rehabilitation, 2004
- Mechanical properties of commercial high strength ceramic core materialsDental Materials, 2004
- Failure analysis of resin composite bonded to ceramicDental Materials, 2003
- In vitro marginal fit of three all-ceramic crown systemsThe Journal of Prosthetic Dentistry, 2003
- Effect of etching and airborne particle abrasion on the microstructure of different dental ceramicsThe Journal of Prosthetic Dentistry, 2003
- Dentin bond strengths of two ceramic inlay systems after cementation with three different techniques and one bonding systemThe Journal of Prosthetic Dentistry, 2003
- Bonding of a mica-based castable ceramic material with a tri-n-butylborane-initiated adhesive resinJournal of Oral Rehabilitation, 1996
- The promotion of adhesion by the infiltration of monomers into tooth substratesJournal of Biomedical Materials Research, 1982