Abstract
Corrosion fatigue crack growth studies have been conducted on a Ni-Cr-Mo-V turbine disc steel in saturated sodium chloride and sodium sulfate environments at 100C. The results show that crack growth rate is accelerated in both the environments at open circuit potential, compared to the rate in air environment. Crack growth rate is further accelerated in both environments with the application of a large cathodic potential. Anodic potential has no effect on crack growth rate relative to that at open circiut potential. Cracking occurred transgranularly around the open circuit potential and intergranularly under severe cathodic charging conditions. The amount of intergranular cracking increased with decreasing frequency in the Cl− environment and occurred predominantly at low ΔK levels. It is suggested that the material cracks by two mechanisms: hydrogen embrittlement at very cathodic potentials, and film rupture and anodic dissolution at relatively noble potentials around the open circuit potential. Finally, comparison of the results with those for concentrated sodium hydroxide (100 C) and double distilled water (97 C) shows that although sodium hydroxide (which is another impurity present in the steam) is the most aggressive specie, distilled water inhances cracking as well. It is recommended that further work be done in high purity water.