Abstract
This study investigates the influence of tungsten (W) deposition on hydrogen plasma-driven permeation (PDP) behavior by examining co-deposition of W and hydrogen on a nickel (Ni) substrate. Experiments were performed using RF plasma sputtering at a substrate temperature of 693 K. The measured hydrogen permeation flux exhibited a transient peak followed by a steady-state phase, even as the W deposition layer continued to grow. Additionally, doubling the Ni substrate thickness had no effect on the steady-state flux, indicating that the permeation was limited by surface recombination processes rather than bulk diffusion. The numerical model was developed to simulate hydrogen diffusion and surface recombination processes in both the Ni substrate and the growing W layer. As W deposition changes the surface condition, the recombination coefficient (Kr) was expressed as a function of time, which successfully reproduced the transient peak observed in the experiment. The temporal suppression of Kr was attributed to the initial deposition of W atoms on the Ni surface. Further validation through repeated discharge experiments with pre-deposited W confirmed that the initial transition from Ni to W was responsible for the peak. These results show that surface changes such as W deposition strongly affect surface recombination, thereby influencing PDP behavior.

This publication has 21 references indexed in Scilit: