Development of AB[sub 2]-Type Zr-Ti-Mn-V-Ni-M Hydride Electrode for Ni-MH Secondary Battery
Authors:
- 1 January 2001
- journal article
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 148 (9) , A1041-A1044
Abstract
A series of multicomponent Zr0.5Ti0.5Mn0.4V0.6Ni0.85M0.15Zr0.5Ti0.5Mn0.4V0.6Ni0.85M0.15 (M = Fe, Co, Cu, Mo, and Al) alloys are prepared and their crystal structure and pressure-composition-temperature curves are examined. The electrochemical properties of these alloys such as discharge capacity, cycling performance, and rate capability are also investigated. Zr0.5Ti0.5Mn0.4V0.6Ni0.85M0.15Zr0.5Ti0.5Mn0.4V0.6Ni0.85M0.15 (M = Fe, Co, Cu, Mo, and Al) alloys have predominantly C14 Laves phases multiple phase structure. The alloys with M = Co and Fe have relatively larger hydrogen storage capacities. The discharge capacities just after activation are relatively large in the case of the alloys with M = Co and Fe. They are 226 and 225 mAh/g, respectively, at the current density 60 mA/g. The Zr0.5Ti0.5Mn0.4V0.6Ni0.85Co0.15Zr0.5Ti0.5Mn0.4V0.6Ni0.85Co0.15 alloy is the best one with a relatively large discharge capacity and good cycling performance. The gradual increases in the discharge capacities of the alloys with the increase in the current density (from 60 to 250 mA/g) are considered to result from the spontaneous hydrogen evolution due to an insufficient hydrogen overvoltage. During activation Ni-rich and Fe-rich regions form on the surface of the Zr0.5Ti0.5Mn0.4V0.6Ni0.85Fe0.15Zr0.5Ti0.5Mn0.4V0.6Ni0.85Fe0.15 alloy. They may act as active sites for the electrochemical reaction. With the increase in the number of charge/discharge cycles for the Zr0.5Ti0.5Mn0.4V0.6Ni0.85Fe0.15Zr0.5Ti0.5Mn0.4V0.6Ni0.85Fe0.15 alloy, the quantities of the zirconium and iron dissolved in the solution increase. © 2001 The Electrochemical Society. All rights reserved.Keywords
This publication has 11 references indexed in Scilit:
- Activation behavior of Zr0.7Ti0.3Cr0.3Mn0.3V0.4Ni alloy electrode modified by the hot-charging treatmentJournal of Alloys and Compounds, 1998
- Electrochemical Properties of Over‐stoichiometric ZrMn1 − x V x Ni1.4 + y Alloys with C15 Laves PhaseJournal of the Electrochemical Society, 1998
- The Ti-based metal hydride electrode for NiMH rechargeable batteriesJournal of Alloys and Compounds, 1996
- Substitution effect of elements in Zr-based alloys with Laves phase for nickel-hydride batteryJournal of Alloys and Compounds, 1995
- A study of the activation behaviour of ZrCrNiLa metal hydride electrodes in alkaline solutionJournal of Alloys and Compounds, 1994
- Activation behaviour of ZrCrNiM0.05 metal hydride electrodes (M La, Mm (misch metal), Nd)Journal of Alloys and Compounds, 1992
- Rechargeable hydrogen batteries using rare-earth-based hydrogen storage alloysJournal of Alloys and Compounds, 1992
- Effects of partial substitution and anodic oxidation treatment of Zr−V−Ni alloys on electrochemical propertiesJournal of the Less Common Metals, 1991
- Electrode characteristics of C15-type laves phasealloysJournal of the Less Common Metals, 1991
- From permanent magnets to rechargeable hydride electrodesJournal of the Less Common Metals, 1987