Fracture Toughness, Fracture Planes and BDT in Stoichiometric Feal and Nial Single Crystals
Authors:
- 1 January 1994
- journal article
- Published by Springer Nature in MRS Proceedings
- Vol. 364
Abstract
Fracture toughness data of stoichiometric FeAl and NiAl single crystals were measured in four-point-bending tests and the crystallographic orientations of the resultant fracture surfaces were determined.For FeAl single crystals unexpectedly high fracture toughness values were measured even at low temperatures (17 MPa [001] at 77K). However, these crystals failed in a brittle manner for temperatures up to 300K. The crystallographic orientation of the fracture surfaces were strongly dependent on the environment due to hydrogen embrittlement.The NiAl specimens were precracked and the fracture toughness was measured in the weakest crystal orientation. The fracture surfaces were similar to those obtained in previous investigations. Although the room temperature (RT) KIC-value was the highest for pure weak-oriented NiAl (7.5 MPa [001]) the BDT temperature was found in the same region where it occurs for the hard orientation (673K to 693K). The onset of the BDT will be discussed.Keywords
This publication has 10 references indexed in Scilit:
- Overview No. 104 The physical and mechanical properties of NiAlActa Metallurgica et Materialia, 1993
- Observation of high index {511} type fracture planes and their influence on toughness in NiAl single crystalsIntermetallics, 1993
- Cleavage fracture in B2 aluminidesActa Metallurgica et Materialia, 1992
- Cleavage fracture of ordered intermetallic alloysMaterials Science and Engineering: A, 1992
- Fracture Mechanisms in Intermetallics1992
- Room temperature fracture of FeAl and NiAlMaterials Characterization, 1991
- NiAl alloys for high-temperature structural applicationsJOM, 1991
- Effect of cooling rate on hardness of FeAl and NiAlMetallurgical Transactions A, 1990
- Brittle fracture and grain boundary chemistry of microalloyed NiAlJournal of Materials Research, 1990
- Anrißerzeugung in WC-Co-Hartmetall-Proben für die Messung des kritischen Spannungsintensitätsfaktors KICMaterialwissenschaft und Werkstofftechnik, 1989