Low-Leakage Tetragonal ZrO2 (EOT < 1 nm) With In Situ Plasma Interfacial Passivation on Germanium

Authors:

Abstract
We successfully fabricated gate stacks (ZrO 2 /GeO x /Ge) with a subnanometer equivalent oxide thickness (EOT) and low-leakage current on n-/p-Ge through plasma-enhanced atomic layer deposition (ALD). A 0.78-nmthick GeOx was formed through plasma oxidation (i.e., in situ plasma interfacial passivation, followed by 3.48-nm-thick ZrO 2 growth in the same ALD reactor). A subnanometer EOT of N0.9 nm was achieved with a relatively high dielectric constant (roughly 30) of tetragonal-phase ZrO 2 . The gate leakage was N1 x 10 -4 A/cm2 at VFB - 1 V, and roughly 5 x 10-5 A/cm2 at VFB t 1 V on pand n-type Ge, respectively. Our ZrO 2 stabilized in the tetragonal phase, when the post-deposition annealing temperature, was higher than 500 °C. Therefore, the proposed scheme is simple and effective for use in pursuing an ultralow EOT gate dielectric on Ge.
Funding Information
  • National Science Council of Taiwan (MOST 104-2119-M-009-008)

This publication has 17 references indexed in Scilit: