The effect of additional photochemical treatments on the bonding of silanized CAD/CAM ceramic restorations after water-storage
Authors:
- 2 January 2021
- journal article
- research article
- Published by Springer Nature in Odontology
- Vol. 109 (3) , 585-595
Abstract
The development of dental CAD/CAM system has made metal-free ceramic restorations more available to patients. Silane coupling treatment is an essential clinical process to achieve reliable and good adhesion with silica-based indirect restoratives. However, long-term water-storage causes the hydrolysis of silane coupling agents and decreases the bond strength. The aim of this study was to examine the effect of additional treatments including photochemical treatments on silane coupling performance in ceramic restorations. The influence of water-storage periods (1d: one day, 1m: one month, and 3m: three months) for the silanized surface of CAD/CAM ceramic restorations was also investigated. In addition, bonding reliability was evaluated as a qualitative measure in order to characterize the bond strength of CAD/CAM restorations. The micro-tensile bond strength (μ-TBS) was measured to explore the benefits of additional photochemical treatments (UV: ultraviolet and VL: visible light irradiations) on silanized surfaces, compared to non-additional treated (CO) and dry heating (DR) conditions. In the CO specimens, μ-TBS decreased in the order of 1d > 1m > 3m. However, in DR, UV, and VL additional treatments, no significant differences could be observed in the 1d, 1m, and 3m groups. The Weibull modulus and 10% failure probability values of the UV and VL specimens were inclined to be significantly greater than those of CO specimens, regardless of the water-storage period. These findings reveal that additional photochemical treatments had a successful effect to improve the bond strength and bonding reliability of the CAD/CAM restorations, when compared to CO and DR conditions.Keywords
This publication has 26 references indexed in Scilit:
- Hydrolytic stability of composite repair bondEuropean Journal of Oral Sciences, 2007
- In Vitro Hydrolytic Degradation of Composite Quartz Fiber-post Bonds Created by Hydrophilic Silane CouplingsOperative Dentistry, 2006
- Effect of post-silanization drying on the bond strength of composite to ceramicThe Journal of Prosthetic Dentistry, 2004
- Conversion of Some Siloxane Polymers to Silicon Oxide by UV/Ozone Photochemical ProcessesChemistry of Materials, 2000
- The analysis of surface degradation on UV-treated epoxy/glass fiber by corona-charging propertiesPolymer Degradation and Stability, 1999
- Effects of Treatment and Storage Conditions on Ceramic/Composite Bond StrengthJournal of Dental Research, 1995
- Relationship between surface area for adhesion and tensile bond strength — Evaluation of a micro-tensile bond testDental Materials, 1994
- Mechanical properties of the glass fibre-polyester interphaseJournal of Materials Science, 1992
- Chemistry of Silane Coupling Agents1991
- Tracer study of kinetics and mechanism of hydrolytically induced interfacial failureJournal of Polymer Science Part C: Polymer Symposia, 1971