HYDRAULIC BINDING AGENT BASED ON SERPENTINITE FROM AMPHIBOLITE DEPOSIT SOKOLOVSKOE
- 19 November 2025
- journal article
- Published by Kola Science Centre in Transaction Kola Science Centre
- Vol. 16 (2) , 248-252
Abstract
The effect of firing temperature of crushed serpentine rock from the Sokolovskoye amphibolite deposit (Sakhalin Region) on the strength of magnesia-silicate binder was studied. It was found that the optimal conditions for obtaining thermally activated serpentinite are firing temperature of 675–725 °C, holding for 25 minutes. Compressive strength of hydraulic binder samples after 28 days of hardening is 5,91–6,15 MPa. Activating additives increase the strength of serpentine binder to 46,7 MPa.Keywords
This publication has 2 references indexed in Scilit:
- NEW FUNCTIONAL ADHESIVES ON THE BASIS OF SERPENTINITEBulletin of the Saint Petersburg State Institute of Technology (Technical University), 2022
- Study of the properties of fine-grained concrete modifiedby the nanodisperse serpentinite additiveVestnik MGSU, 2013