Extended Defects in ZnO Ceramics Containing Bi 4 Ti 3 O 12 Additive
Authors:
- 1 May 1994
- journal article
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 77 (5) , 1202-1208
Abstract
Extended defects in ZnO ceramics containing, 6 wt% Bi 4 Ti 3 O 12 were studied by analytical electron microscopy. Apart from basal plane condensation stacking faults, which are also present in as‐received ZnO, extended defects related to the presence of Bi 4 Ti 3 O 12 were observed. In samples sintered at 900°C they lie in the basal or in the prismatic planes and they quite often form closed loops, whereas they form serpentine‐shaped boundaries in samples sintered at 1200°C. Evidence is given that they are inversion boundaries. Their TEM image characteristics, as well as the unambiguous presence of Ti at the boundaries, suggest that they are formed due to the presence of 2‐D coherent precipitates of Ti‐rich (possibly Zn 2 TiO 4 ‐type spinel) phase.Keywords
This publication has 23 references indexed in Scilit:
- Chemistry of Basal Plane Defects in Zinc Oxide–Antimony Oxide (0.1 mol%) CeramicsJournal of the American Ceramic Society, 1992
- Grain Growth of Zinc Oxide During the Sintering of Zinc Oxide—Antimony Oxide CeramicsJournal of the American Ceramic Society, 1991
- Inversion Domains in Aluminum NitrideJournal of the American Ceramic Society, 1991
- Transmission Electron Microscope Study of Antimony‐Doped Zinc Oxide CeramicsJournal of the American Ceramic Society, 1991
- On the structure of faulted interfaces in aluminium nitride ceramicsPhilosophical Magazine A, 1991
- Twinning in ZnO Ceramics with Sb2O3 AdditionsJournal of the Ceramic Society of Japan, 1991
- Inversion Twin Boundaries in Zinc OxideJournal of the American Ceramic Society, 1990
- Grain Growth in Sintered ZnO and ZnO‐Bi 2 O 3 CeramicsJournal of the American Ceramic Society, 1990
- Extended defects in sintered AINJournal of Materials Science, 1989
- Surface polarity and symmetry in semiconducting compoundsJournal of Materials Science, 1988