Effect of coupling agent quantity on composite interface structure and properties of fiber metal laminates
Authors:
- 4 April 2021
- journal article
- research article
- Published by Wiley in Polymer Composites
- Vol. 42 (7) , 3195-3205
Abstract
Epoxy silane coupling agent A‐187 and amine silane coupling agent A‐1387 were used to modify the interface of carbon‐reinforced aluminum laminates (CARE), respectively. The effects of the type and content of coupling agent on the microstructure and mechanical properties of CARE were investigated. Results show that with the increase in the content of two coupling agents, the wettability first increases and then decreases. When the mass fraction of the two coupling agents is 1%, good wetting property is obtained, and the interlaminar shear and flexural strengths of the CARE plate are the best. Compared with epoxy coupling agent A‐187, amine coupling agent A‐1387 had better wettability to aluminum alloy surface and highly contributed to the improvement of interface structure and properties, which then increased the interlaminar shear and flexural strengths by 19.1% and 8.9%, respectively.Keywords
This publication has 16 references indexed in Scilit:
- Direct joining of carbon-fiber–reinforced plastic to an aluminum alloy using friction lap joiningComposites Part B: Engineering, 2015
- Characteristics and formation mechanism of porosities in CFRP during laser joining of CFRP and steelComposites Part B: Engineering, 2015
- Surface modifications of Ti alloy with tunable hierarchical structures and chemistry for improved metal–polymer interface used in deepwater composite riserApplied Surface Science, 2015
- Adhesive–embossing Hybrid Joining Process to Fiber-reinforced Thermosetting Plastic and Metallic Thin SheetsProcedia Engineering, 2014
- Low velocity impact response of fibre-metal laminates – A reviewComposite Structures, 2014
- Surface microstructures and epoxy bonded shear strength of Ti6Al4V alloy anodized at various temperaturesComposites Science and Technology, 2013
- A review: Fibre metal laminates, background, bonding types and applied test methodsMaterials & Design (1980-2015), 2011
- Enhancement of composite‐metal interfacial adhesion strength by dendrimerSurface and Interface Analysis, 2011
- Effect of processing parameters on pore structure and thickness of anodic aluminum oxide (AAO) tubular membranesJournal of Membrane Science, 2008
- Effects of anodizing conditions on anodic alumina structureJournal of Materials Science, 2007