A Study of Beta Processing of Ti-6Al-4V: Is it Trivial?
Authors:
- 1 March 2001
- journal article
- Published by ASME International in Journal of Engineering Materials and Technology
- Vol. 123 (3) , 355-360
Abstract
Deformation of Ti-6Al-4V alloy in the β phase field is generally considered to be trivial since the material is highly workable at these temperatures and does not normally pose problems during processing. In view of this, studies on the hot deformation behavior of β are scanty compared to those on the α−β deformation. This paper is focussed on understanding the β deformation characteristics in Ti-6Al-4V with a view to examine whether such studies help in optimizing the process design and achieving microstructural control. The emphasis has been on the two industrial grades, viz. commercial purity (CP) versus extra-low interstitial (ELI), and also on the effect of starting microstructure (transformed β versus equiaxed α+β). The stress-strain curves obtained in compression exhibited steady-state behavior at strain rates lower than 1 s−1 and oscillatory/softening behavior at higher strain rates. Kinetic analysis of the flow stress data obtained at different temperatures and strain rates has shown that the stress exponent is about 3.6-3.8 and the apparent activation energy is in the range 150-287 kJ/mole, which is comparable to that of self-diffusion in β phase (150 kJ/mol). Dynamic recrystallization (DRX) of β is identified as the microstructural mechanism in all the cases except in ELI grade with transformed β starting structure. The prior β grain size in the DRX region exhibits a good correlation with the Zener-Hollomon parameter. In case of ELI grade, a mechanism of large grained superplasticity involving sliding of prior colony boundaries has been identified. However, deformation close to the transus in ELI grade causes nucleation of voids which may grow during soaking at the deformation temperature under the influence of tensile residual stress. The results clearly show that a study of β deformation mechanisms holds the key during hot working of Ti-6-4. More importantly, the processing schedule used for CP grade Ti-6-4 should not be used for ELI grade to achieve microstructural control and avoid defects.Keywords
This publication has 23 references indexed in Scilit:
- Unstable flow during supratransus working of Ti–6Al–4VMaterials Letters, 2001
- Influence of oxygen content on the forging response of equiaxed (α+β) preform of Ti–6Al–4V: commercial vs. ELI gradeJournal of Materials Processing Technology, 2000
- Microstructural Modeling and Process Control During Hot Working of Commercial Ti-6A1-4V: Response of Lamellar and Equiaxed Starting MicrostructuresMaterials and Manufacturing Processes, 2000
- Hot working of commercial Ti–6Al–4V with an equiaxed α–β microstructure: materials modeling considerationsMaterials Science and Engineering: A, 2000
- Hot deformation and microstructural damage mechanisms in extra-low interstitial (ELI) grade Ti–6Al–4VMaterials Science and Engineering: A, 2000
- Physical processes and regimes of thermomechanical processing controlling development of regulated structure in the α+β titanium alloysMaterials Science and Engineering: A, 1998
- Modelling of hot deformation for microstructural controlInternational Materials Reviews, 1998
- Other possible superplasticity mechanisms1997
- Superplastic deformation characteristics of microduplex Ti–6Al–4V alloyMaterials Science and Technology, 1986
- Strength and structure under hot-working conditionsInternational Materials Reviews, 1969