Precursor Powders for Sulfide Ceramics Prepared by Evaporative Decomposition of Solutions
Authors:
- 1 November 1983
- journal article
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 66 (11) , c205-c206
Abstract
Precursor oxide powders for the synthesis of ternary sulfide ceramics can be prepared by the evaporative decomposition of nitrate solutions. The oxides can be sulfidized inflowing H,S at 1000 C with little grain growth. Ceramics prepared by direct sintering of these powders in flowing H0S have a much lower porosity than ceramics prepared from conventionally fired powders and sintered under identical conditions. Particle sizes are in the micrometer size range, in agreement with calculation .Keywords
This publication has 4 references indexed in Scilit:
- Processing Ternary Sulfide Ceramics: Powder Preparation, Sintering, and Hot‐PressingJournal of the American Ceramic Society, 1983
- CaLa2S4: Ceramic Window Material For The 8 to 14 μm Region1982
- The System CaO‐Al 2 O 3 ‐H 2 OJournal of the American Ceramic Society, 1956
- Atomization of Liquids in High Velocity Gas StreamsIndustrial & Engineering Chemistry, 1948