Kinetics of Hydrogen Formation from Mild Steel in Water under Anaerobic Conditions
Authors:
- 1 February 1982
- journal article
- Published by Association for Materials Protection and Performance (AMPP) in Corrosion
- Vol. 38 (2) , 98-104
Abstract
The effect of copper (metallic and up to 1 ppm. dissolved in solution), temperature (60 C to 90 C), and pH (6 to 9) on hydrogen formation from mild steel in oxygen free water was investigated. The formation rate was found Independent of temperature not only up to 90 C, but a comparison with work elsewhere indicates that this observation applies over a much wider temperature range. Copper was found to have had no practical catalytic effect upon the hydrogen formation rate. The volumetric rate of hydrogen evolution was qualitatively proportional to weight loss, though not all hydrogen expected from stoichiometric considerations appeared as free gas. There was no clear evidence that black magnetite (Fe3O4) was the only solid corrosion product.Keywords
This publication has 17 references indexed in Scilit:
- Corrosion of a cast iron boiler in a model central heating systemCorrosion Science, 1978
- On the catalytic effect of certain metals on the corrosion of iron in oxygen-free waterCorrosion Science, 1978
- The thermodynamic consideration for Fe-H2O system at 25°CCorrosion Science, 1973
- A study of some products of the corrosion of Fe under hydrothermal conditions using the Mössbauer effectCorrosion Science, 1971
- Stability of ferrous hydroxide in aqueous suspension at 300°cJournal of Chemical Technology & Biotechnology, 1967
- The corrosion of mild steel in boiling salt solutionsCorrosion Science, 1967
- The mechanism of formation of a porous oxide film on steelCorrosion Science, 1966
- The de‐aeration of aqueous solutionsJournal of Chemical Technology & Biotechnology, 1962
- Stability of Ferrous Hydroxide PrecipitatesThe Journal of Physical Chemistry, 1956
- Evolution of Hydrogen from Ferrous HydroxideNature, 1948